Elektrode Bir ah oo AWS E7015-A1 ah oo Kulayl-u-adkaysi u leh R107 Ulaha Alxanka Haydarojiin Yar

Sharaxaad Gaaban:

R107 (AWS E7015-A1) waa elektarood bir ah oo kulaylka u adkaysta oo leh dahaar sodium oo haydarojiin yar leh oo ka kooban 0.5% Mo.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Birta u adkaysta kulaylka ee Molybdenum iyo ChromiumAlxankaElektrode

R107                                                     

GB/T E5015-A1

AWS A5.5 E7015-A1

Sharaxaad: R107 waa elektarood bir ah oo kulaylka u adkaysta oo leh dahaar sodium oo haydarojiin yar leh oo ka kooban 0.5% Mo. Isticmaal DCEP (elektaroodka hadda jira ee tooska ah ee wanaagsan) waxaana lagu dhejin karaa dhammaan boosaska. Alxanka waa in la kululeeyaa ilaa 90 ~ 110 ℃ ka hor inta aan la alxanka.

Adeegsiga: Waxaa loo isticmaalaa tuubooyinka kuleeliyaha alxanka leh heerkulka shaqada oo ka hooseeya 510°C (sida 15Mo, iwm.), waxaana sidoo kale loo isticmaali karaa alxanka guud ee birta xoogga badan ee daawaha hooseeya.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Mo

S

P

≤0. 12

0.50 ~ 0.90

≤0.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Sifooyinka farsamada ee birta alxanka:

Shayga tijaabada ah

Xoogga jiidista

Mpa

Xoogga wax soo saarka

Mpa

Kordhinta

%

Qiimaha saameynta (J)

Heerkulka Caadiga ah.

Dammaanad qaaday

≥490

≥390

≥22

≥47

 

Fidinta haydarojiin ee birta la dhigay: ≤6.0mL/100g (habka glycerin)

Baarista raajada: Darajada I

 

Hadda lagu taliyay:

Dhexroorka usha

(mm)

2.0

2.5

3.2

4.0

5.0

Hadda alxanka

(A)

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Ogeysiis:

1. Elektroodka waa in la dubo 1 saac heerkul ah 350℃ ka hor inta aan la isticmaalin alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda ku jirta qaybaha alxanka ka hor inta aan la alxanka.