Nikel Alloy Welding Wire ERNiCrMo-3 Mig Welding Wire

Sharaxaad Gaaban:

ERNiCrMo-3 waa silig daawaha nikkel sare ah oo loo sameeyay alxanka iyo dahaadhka nikkel-ku-salaysan sida 625 ama walxo la mid ah.


Faahfaahinta Alaabta

Tags Product

Alloy NickelXargaha alxankaERNiCrMo-3

 

Heerarka

EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb

AWS A5.14 - ER NiCrMo-3

 

Tilmaamaha iyo Codsiyada

Sarenikkelsilig daawaha ah oo loo sameeyay alxanka iyo isku dhejintanikkelAlloys-ku salaysan sida 625 ama wax la mid ah.

Adag oo loo sawiray hab gaar ah si loo helo alxanka nadiifka ah iyo tayada sare leh oo leh tol dhalaalaya iyo ductility heer sare ah.

Birta alxanka waxay leedahay sifooyin farsamo oo aad u wanaagsan oo heerkul sarreeya iyo mid hooseeya.

Iska caabbinta wanaagsan ee godka iyo daxalka walbahaarka.

Heerkulka shaqada ee lagu taliyay wuxuu u dhexeeyaa cryogenic ilaa 540°C.

Nabarka lakabka saxda ah ee sifooyinka quudinta siliga sare.

Caadi ahaan loo isticmaalo warshadaha habka kiimikada, injineernimada badda, qaybaha reactor nukliyeerka, hawada hawada iyo gudaha qalabka xakamaynta wasakhowga iwm.

 

Qalabka Saldhigga Caadiga ah

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926* * Illustrative, aan ahayn liis dhamaystiran

 

Halabuurka Kiimikada %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

Min

1.0

0.40

0.40

23.00

4.15

10.00

 

Guryaha Makaanikada

Xoogga Jilicsan

≥760 MPa

Xoogga Wax-soo-saarka

≥415 MPa

Dheeraynta

≥35%

Xoogga Saamaynta

≥100 J

Guryaha makaanikada waa qiyaas waxayna ku kala duwanaan karaan kuleylka, gaaska gaashaanka, cabbirada alxanka iyo arrimo kale.

Gaasaska gaashaanka

TS EN ISO 14175 - I1, I3

Goobaha alxanka

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF

Xogta Baakadaha

Dhexroorka

Miisaanka

Spool

Pallet Qty

1.00 mm

1.20 mm

15 Kg

15 Kg

BS300

BS300

72

72

Mas'uuliyadda:In kasta oo dhammaan dadaallo macquul ah la sameeyay si loo hubiyo saxnaanta macluumaadka ku jira, macluumaadkan waa la beddeli karaa ogeysiis la'aan waxaana loo qaadan karaa oo keliya inay ku habboon tahay hagidda guud.