ER4043 waa silig alxanka aluminiumka ah oo ujeedo guud leh. Waa mid ka mid ah alxanka iyo alxanka ugu da'da weyn uguna isticmaalka badan. Alxankan aluminiumka ah waxa ku jira waxyaabo lagu daro silicon, kuwaas oo keena dheecaan wanaagsan (ficil qoyn) oo barkadda alxanka ah waxayna sidoo kale soo saartaa alxan aan xasaasiyad ku lahayn dildilaaca. Dhammaadkeeda alxanka dhalaalaya ayaa ka dhigaya mid caan ah oo alxanayaasha ah. ER4043 waxaa loo isticmaali karaa in lagu alxanka noocyo kala duwan oo aluminium ah.
Codsiyada Caadiga ah: silig buuxin alxanka; buufin iyo silig bir-birta ololka ah
| Fasalka AWS: ER4043 | Shahaadada: AWS A5.10/ A5.10M:1999 |
| Daawaha: ER4043 | AWS/ASME SFA A5.10 |
| Booska Alxanka: F, V, OH, H | Hadda: DCEP-GMAW AC-GTAW |
Sifooyinka Caadiga ah (sida loo welded)
| Gudbinta: | 42% IACS (-12) |
| Xoogga jiidista, kpsi: | 29 |
| Midabka: | Cawlan |
| Barta Dhalmada | 1170⁰F | Adkaynta | 1065⁰F | Cufnaanta | 0.097 lbs/cu Gudaha. |
Kiimikada Wire-ka Caadiga ah sida ku xusan AWS A5.10 (qiimayaasha hal-hal ah ayaa ugu badan)
| Si | Fe | Cu | Mn | Mg | Zn | Ti | Kale | Al | ||||||
| 4.5-6.0 | 0.8 | 0.30 | 0.05 | 0.05 | 0.10 | 0.20 | 0.15 | Haraadiga | ||||||
| Halbeegyada Alxanka Caadiga ah | ||||||||||||||
| Dhexroorka | Geedi socodka | Volt | Amps | Gaas | ||||||||||
| in | (mm) | |||||||||||||
| .030 | (.8) | GMAW | 15-24 | 60-175 | Argon (cfh) | |||||||||
| .035 | (.9) | GMAW | 15-27 | 70-185 | Argon (cfh) | |||||||||
| 3/64” | (1.2) | GMAW | 20-29 | 125-260 | Argon (cfh) | |||||||||
| 1/16” | (1.6) | GMAW | 24-30 | 170-300 | Argon (cfh) | |||||||||
| 3/32” | (2.4) | GMAW | 26-31 | 275-400 | Argon (cfh) | |||||||||
| Dhexroorka | Geedi socodka | Volt | Amps | Gaas | ||||||||||
| in | (mm) | |||||||||||||
| 1/16” | (1.6) | GTAW | 15 | 60-80 | Argon (cfh) | |||||||||
| 3/32” | (2.4) | GTAW | 15 | 125-160 | Argon (cfh) | |||||||||
| 1/8” | (3.2) | GTAW | 15 | 190-220 | Argon (cfh) | |||||||||
| 5/32” | (4.0) | GTAW | 15 | 200-300 | Argon (cfh) | |||||||||
| 3/16” | (4.8) | GTAW | 15-20 | 330-380 | Argon (cfh) | |||||||||
Shirkadda Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanayn soo saarista elektroodhada alxanka, ulaha alxanka, iyo waxyaabaha la isticmaalo ee alxanka in ka badan 20 sano.
Waxyaabaha ugu muhiimsan ee aan ka sameyno waxaa ka mid ah elektroodhada alxanka birta aan la saarin, elektroodhada alxanka birta kaarboon, elektroodhada alxanka birta aan la jarin, elektroodhada alxanka dusha sare, elektroodhada alxanka birta aan la jarin ee nickel & cobalt, fiilooyinka alxanka birta aan la jarin ee khafiifka ah & hoose, fiilooyinka alxanka birta aan la jarin, fiilooyinka flux ee gaaska lagu gaashaamiyay, fiilooyinka alxanka aluminium, fiilooyinka alxanka arc ee hoos yimaada, fiilooyinka alxanka nickel & cobalt ee birta, fiilooyinka alxanka naxaasta ah, fiilooyinka alxanka TIG & MIG, elektroodhada tungsten, elektroodhada kaarboon ee gouging, iyo agabyada kale ee alxanka & waxyaabaha la isticmaalo.