ER5356 Alxanka Aluminium-ka ah Ulaha Alxanka iyo Elektroodhada

Sharaxaad Gaaban:

ER5356 waa daawaha aluminiumka ah ee loogu talagalay ujeedo guud kaas oo badanaa loo doorto xooggiisa xiirashada oo sarreeya.


Faahfaahinta Badeecada

Calaamadaha Alaabta

ER5356 waa nooc aluminium ah oo loogu talagalay ujeedo guud kaas oo badanaa loo doorto xooggiisa xiirashada oo sarreeya. Intaa waxaa dheer, waxay sidoo kale bixisaa iska caabin aad u fiican oo daxalka ah marka la taabto biyo milix leh. ER5356 waa in la tixgeliyaa marka la alxamayo biraha salka aluminium ee taxanaha ah ee 5000.

Codsiyada Caadiga ah: silig buuxinta alxanka

Fasalka AWS: ER5356 Shahaadada: AWS A5.10/ A5.10M:1999
Daawaha: ER5356 AWS/ASME SFA A5.10
Booska Alxanka:
F, V, OH, H
Hadda:
DCEP-GMAW
AC-GTAW
Sifooyinka Caadiga ah (sida loo welded)
Gudbinta: 29% IACS (-0)/27% IACS (-H18)
Xoogga jiidista, kpsi: 38
Midabka: Caddaan
Barta Dhalmada 1175⁰F Adkaynta 1060⁰F Cufnaanta 0.096 lbs/cu Gudaha.
Kiimikada Wire-ka Caadiga ah sida ku xusan AWS A5.10 (qiimayaasha hal-hal ah ayaa ugu badan)
Si Fe Cu Mn Mg Cr Zn Ti Kale AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Haraadiga
Halbeegyada Alxanka Caadiga ah
Dhexroorka Geedi socodka Volt Amps Gaas
in (mm)
.030 (.8) GMAW 15-24 60-175 Argon (cfh)
.035 (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argon (cfh)
Dhexroorka Geedi socodka Volt Amps Gaas
in (mm)
1/16” (1.6) GTAW 15 60-80 Argon (cfh)
3/32” (2.4) GTAW 15 125-160 Argon (cfh)
1/8” (3.2) GTAW 15 190-220 Argon (cfh)
5/32” (4.0) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

Shirkadda Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanayn soo saarista elektroodhada alxanka, ulaha alxanka, iyo waxyaabaha la isticmaalo ee alxanka in ka badan 20 sano.

Waxyaabaha ugu muhiimsan ee aan ka sameyno waxaa ka mid ah elektroodhada alxanka birta aan la saarin, elektroodhada alxanka birta kaarboon, elektroodhada alxanka birta aan la jarin, elektroodhada alxanka dusha sare, elektroodhada alxanka birta aan la jarin ee nickel & cobalt, fiilooyinka alxanka birta aan la jarin ee khafiifka ah & hoose, fiilooyinka alxanka birta aan la jarin, fiilooyinka flux ee gaaska lagu gaashaamiyay, fiilooyinka alxanka aluminium, fiilooyinka alxanka arc ee hoos yimaada, fiilooyinka alxanka nickel & cobalt ee birta, fiilooyinka alxanka naxaasta ah, fiilooyinka alxanka TIG & MIG, elektroodhada tungsten, elektroodhada kaarboon ee gouging, iyo agabyada kale ee alxanka & waxyaabaha la isticmaalo.

 

 