Nikkel DaawahaSilig alxankaWire Tig ahERNiFeCr-1
| Heerarka |
| TS EN ISO 18274 - Ni 8065 - NiFe30Cr21Mo3 |
| AWS A5.14 – ER NiFeCr-1 |
Sifooyinka iyo Codsiyada
Daawaha 825 waanikkel-fiilada birta-chromium taasoo ka dhigaysa doorasho ku habboon codsiyo kala duwan oo adag.
Siliggan wuxuu bixiyaa heer sare oo iska caabin ah oo daxalka ah si uu u yareeyo oksaydheynta iyo deegaanka oo yaraada labadaba.
Ku habboon dahaarka dusha sare leh halkaas oo loo baahan yahay isku-darka kiimikada oo la mid ah.
Alxan aad u fiican oo leh bir alxan oo si buuxda u austenitic ah oo leh iska caabin sare oo ka dhan ah dildilaaca daxalka ee warbaahinta ay ku jiraan ion-yada koloriin.
Caadi ahaan waxaa loo isticmaalaa warshadaha kiimikada, kiimikada batroolka, wax soo saarka waraaqaha iyo korontada iwm.
Qalabka Saldhigga Caadiga ah
G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, Alloy 825, N08028, UNS N08825 W.Nr: 1.4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465, 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* Liis tusaale ah, oo aan dhammaystirnayn
| Halabuurka Kiimikada % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | |
| ugu badan | 0.70 | 22.00 | ugu badan | ugu badan | ugu badan | |
| 0.05 | 0.90 | daq | 0.020 | 0.004 | 0.50 | |
|
|
|
|
|
|
| |
| Cu% | Ni% | Al% | Ti% | Cr% | Bisha% | |
| 2.30 | 43.00 | ugu badan | 1.00 | 22.00 | 3.00 | |
| 3.00 | 46.00 | 0.20 | 1.20 | 23.50 | 3.50 | |
| Sifooyinka Farsamada | ||
| Xoogga Tijaabada | ≥550 MPa | |
| Xoogga Wax Soo Saarka | - | |
| Kordhinta | - | |
| Xoogga Saamaynta | - | |
Sifooyinka farsamoyaqaanku waa qiyaas waxayna ku kala duwanaan karaan iyadoo lagu saleynayo kulaylka, gaaska gaashaamaynta, xuduudaha alxanka iyo arrimo kale.
Gaasaska gaashaanka
TS EN ISO 14175 - TIG: I1 (Argon)
Meelaha Alxanka
TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG
| Xogta Baakaynta | |||
| Dhexroorka | Dhererka | Miisaanka | |
| 1.60 mm 2.40 mm 3.20 mm | 1000 mm 1000 mm 1000 mm | 5 Kg 5 Kg 5 Kg | |
Mas'uuliyadda: Iyadoo dhammaan dadaallada macquulka ah la sameeyay si loo hubiyo saxnaanta macluumaadka ku jira, macluumaadkan waa la beddeli karaa iyada oo aan la ogeysiin waxaana loo tixgelin karaa oo keliya inuu ku habboon yahay hagitaan guud.