Waxaan aaminsanahay: Hal-abuurku waa nafteenna iyo ruuxeenna. Tayada wanaagsani waa nolosheenna. Baahida loo qabo in wax iibsadeyaashu ay tahay Ilaaheenna si loogu helo warshad qiimo jaban oo warshadeed oo u adkaysta daxalka birta yar ee birta ah (AWS E8016-G), Waxaan raadineynay inaan horumarinno xiriir iskaashi oo aan kula yeelanno. Xasuuso inaad nala soo xiriirto si aad u hesho faahfaahin dheeraad ah.
Waxaan aaminsanahay: Hal-abuurku waa nafteenna iyo ruuxeenna. Tayada wanaagsani waa nolosheenna. Baahida loo qabo in wax iibsadeyaashu ay tahay Ilaaheenna.Daxalka Shiinaha ee iska caabbinta birta daawaha yarWaxaan kugu soo dhaweyneynaa inaad booqato shirkaddayada iyo warshadeenna. Sidoo kale waa ku habboon tahay inaad booqato boggayaga internetka. Kooxdayada iibka ayaa ku siin doonta adeegga ugu fiican. Haddii aad u baahan tahay macluumaad dheeraad ah, xasuuso inaad xor u tahay inaad nagala soo xiriirto emayl ama taleefan. Waxaan si daacad ah u rajeyneynay inaan xiriir ganacsi oo wanaagsan kula yeelano fursaddan, oo ku salaysan faa'iido siman laga bilaabo hadda ilaa mustaqbalka.
CODSIYADA:
Alxanka birta 9% Cr-1% Mo iyo 9% Cr - 2% Mo oo loo isticmaalo korontada iyo weelka cadaadiska sare leh.
SHARAXAADA:
PA-8016-B8 waa elektarood haydarojiin hooseeya oo birta alxanka ay ka kooban tahay 9%Cr-1%Mo. Waxaa loogu talagalay birta heerkulka sare leh iyo biraha adeegyada haydarojiinta kulul, gaar ahaan warshadaha batroolka. Elektaroodku waxaa loo ansixin karaa xooggiisa sare ee la jiidi karo, adkaysigiisa wanaagsan iyo iska caabbinta kulaylka oo weyn.
OGAYSIIS KU SAABSAN ISTICMAALKA:
1. Elektroodhada ku qallaji 350-400°C ilaa hal saac ka hor isticmaalka oo elektroodhada ku kaydi 100-150°C ka dib markaad qalajiso si taxaddar leh si aad uga fogaato qoyaanka.
2. Ku dhaqan habka tallaabada dambe ama ku dhufo qaansada saxan bir ah oo yar oo loo diyaariyey ujeeddadan gaarka ah si looga hortago in godadku ay bilaabaan qaansada.
3. Qaanso-garee sida ugu macquulsan u gaabi.
4. Kuleyli 100-150°C. Heerkulka la marinayo wuu kala duwan yahay iyadoo la raacayo dhumucda saxanka iyo nooca birta la isku dhejinayo.
5. Fiiro gaar ah u yeelo inaadan dhaafin kuleylka saxda ah sababtoo ah kulaylka xad-dhaafka ah wuxuu sababaa hoos u dhaca qiimaha saameynta iyo xoogga wax-soo-saarka birta alxanka.
IV. QAYBTA KIIMIKADA CAADIGA AH EE BIRTA ALXAMDIGA (%):
| C | Si | Mn | Cr | Mo |
| 0.06 | 0.42 | 0.68 | 9.38 | 1.05 |
V. ASTAAMAHA MAKAANIKADA CAADIGA AH EE BIRTA ALXAN:
| Xoogga Tijaabada N/mm2(Ksi) | Barta Wax-soo-saarka N/mm2 (Ksi) | Kordhinta % | PWHT |
| 705 (102) | 560 (81) | 24 | 740°C x 1 saac |
VI. BOOSKA ALXANAHA: DHAMMAAN BOOSASKA
VII. CABBIRKA IYO BAAXADA HADDA LAGU TALINAYO (AC/DC+):
| Dhexroorka (mm) | 2.5 | 3.2 | 4.0 | 5.0 | |
| Dhererka (mm) | 350 | 350 | 400 | 400 | |
| Ampere | Fidsan | 55 – 85 | 90 - 130 | 130 - 180 | 180 - 240 |
| V & OH | 50 - 80 | 80 - 115 | 110 - 170 | 150 - 200 |
Waxaan aaminsanahay: Hal-abuurku waa nafteenna iyo ruuxeenna. Tayada wanaagsani waa nolosheenna. Baahida loo qabo in wax iibsadeyaashu ay tahay Ilaaheenna si loogu helo warshad qiimo jaban oo warshadeed oo u adkaysta daxalka birta yar ee birta ah (AWS E8016-G), Waxaan raadineynay inaan horumarinno xiriir iskaashi oo aan kula yeelanno. Xasuuso inaad nala soo xiriirto si aad u hesho faahfaahin dheeraad ah.
Warshadda qiimaha jabanDaxalka Shiinaha ee iska caabbinta birta daawaha yarWaxaan kugu soo dhaweyneynaa inaad booqato shirkaddayada iyo warshadeenna. Sidoo kale waa ku habboon tahay inaad booqato boggayaga internetka. Kooxdayada iibka ayaa ku siin doonta adeegga ugu fiican. Haddii aad u baahan tahay macluumaad dheeraad ah, xasuuso inaad xor u tahay inaad nagala soo xiriirto emayl ama taleefan. Waxaan si daacad ah u rajeyneynay inaan xiriir ganacsi oo wanaagsan kula yeelano fursaddan, oo ku salaysan faa'iido siman laga bilaabo hadda ilaa mustaqbalka.