Elektrode Alxanka oo adag DIN 8555 (E10-UM-65-GRZ) Usha Alxanka ee dusha sare Lambarka Nooca: TY-C LEDURIT 67 Usha Alxanka ee Arc

Sharaxaad Gaaban:

DIN 8555 (E10-UM-65-GRZ) waa elektarood SMAW ah oo dahaar sare leh oo loogu talagalay dahaarka adag.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Elektrode Alxanka oo adag

 

Heerka: DIN 8555 (E10-UM-65-GRZ)

Nooca Lambarka: TY-C LEDURIT 67

 

Qeexitaanka & Codsiga:

· Elektroodka SMAW ee dib u soo kabashada sare leh ee aasaasiga ah ee loogu talagalay dahaarka adag.

· Dusha sare ee adag ee qaybaha oo xoqid culus iyo saameyn dhexdhexaad ah maraya.

· Ku habboon lakabka adag ee ugu dambeeya ka dib lakabka kaydka.

· Qaybaha warshadda Sinter, baararka xirashada iyo saxamada, baararka xoqidda, foornada qaraxa, nidaamyada dallacaadda, foornada sibidhka, ilkaha iyo bushimaha baaldiga, shaashadaha.

 

Halabuurka kiimikada ee biraha la shubay(%):

 

C

Si

Mn

Cr

B

DIN

Maaddada C ee Sare iyo Maaddada C

Caadi ah

3.5

1.0

1.8

35

1.0

 

Adkaanta birta la shubay:

deebaaji alxan saafi ah

(HRC)

1 lakab oo ku yaal 0.15% bir ah

(HRC)

2 lakab oo ku yaal 0.15% bir ah

(HRC)

62 – 65

59 – 63

61 – 64

 

Astaamaha Guud:

· Qaab-dhismeedka Yar-yar ee Martensitic+Austenite+Carbides

· Shiidida Mashiinka oo keliya

· Ku dhaqidda Redry muddo 2 saacadood ah heerkul ah 300℃ ka hor inta aan la isticmaalin.


  • Kii hore:
  • Xiga: