Elektrode-ka Birta Daawaha Yar J506NiMA、J507NiMA GB/T E5016-G E5015-G AWS E7018-G E7015-G

Sharaxaad Gaaban:

J506NiMA (AWS E7018-G) iyo J507NiMA (AWS E7015-G) waa elektroodhyo bir ah oo aad u hooseeya oo dahaadh-haydarojiin ah oo leh dahaadh-hoose.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Elektrode-ka Alxanka Birta ee Yar

J506NiMA、J507NiMA                                                     

GB/T E5016-G E5015-G

AWS E7018-G E7015-G

Sharaxaad: J506NiMA iyo J507NiMA waa elektroodhyo bir ah oo aad u hooseeya oo hydrogen-ku dahaaran oo leh dahaadh yar. Birta la dhigay waxay leedahay balaastik aad u fiican, adkaysi heerkul hoose iyo iska caabin dildilaac, waxaana lagu dhejin karaa meel kasta. Dahaarka waa mid u adkaysta nuugista qoyaanka. Ka dib marka elektroodka lagu dubo 400°C x 1 saac oo la dhigo jawi leh qoyaan qaraabo ah ≥ 80% muddo 4 saacadood ah, qoyaanka dahaarka ayaa weli buuxinaya shuruudaha isticmaalka.

Codsiga: Waxaa loo isticmaalaa alxanka goobaha saliidda, maraakiibta, maraakiibta cadaadiska, iyo dhismayaasha kale ee laga sameeyaybirta kaarboonka iyo birta daawaha yar.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Ni

S

P

Dammaanad qaaday

≤0. 12

≥1.00

≤0.50

≤0.60

≤0.035

≤0.040

 

Sifooyinka farsamada ee birta alxanka:

Shayga tijaabada ah

Xoogga jiidista

Mpa

Xoogga wax soo saarka

Mpa

Kordhinta

%

Qiimaha saameynta (J)

-46℃

Dammaanad qaaday

≥490

≥390

≥22

≥27

 

Fidinta haydarojiin ee biraha la dhigay: ≤5.0mL/100g (habka koromatografiga gaaska ama meerkuriga)

Qoyaanka dahaarka elektroodka: ≤0.30%

Baarista raajada: Darajada I

 

Hadda lagu taliyay:

Dhexroorka usha

2.5

3.2

4.0

5.0

Hadda alxanka

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Ogeysiis:

1. Elektroodka waa in la dubo 1 saac heerkul ah 350 ~ 400℃ ka hor inta aan la isticmaalin alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda ku jirta qaybaha alxanka ka hor alxanka;

3. Adeegso hawlgal qaanso gaaban marka aad alxanayso. Jidka alxanka cidhiidhiga ah waa mid habboon.

 