Nikkel DaawahaSilig alxankaWire Tig ahERNi-1
| Heerarka |
| EN ISO 18274 - Ni 2061 - NiTi3 |
| AWS A5.14 – ER Ni-1 |
Sifooyinka iyo Codsiyada
ER-Ni1 waxaa loo isticmaalaa alxanka iyo dahaarka birta Nickel 200 iyo Nickel 201.
Ku habboon in lagu daro birta birta ah ee Monel iyo naxaasta-nikkelbirta kaarboonka ah ee birta ah.
Ni1 wuxuu ka kooban yahay titanium ku filan si loo xakameeyo daloolka birta alxanka ee hababka alxanka.
Badanaa waxaa loo isticmaalaa warshadaha kiimikada, wax soo saarka faybarka synthetic-ga iyo qalabka cuntada lagu sameeyo iwm.
Qalabka Saldhigga Caadiga ah
Nikkel 200 iyo 201*
* Liis tusaale ah, oo aan dhammaystirnayn
| Halabuurka Kiimikada % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | |
| ugu badan | ugu badan | ugu badan | ugu badan | ugu badan | ugu badan | |
| 0.05 | 0.80 | 0.70 | 0.030 | 0.010 | 0.75 | |
| Cu% | Ni% | Co% | Ti% | Al% | ||
| ugu badan | 93.00 | ugu badan | 2.00 | ugu badan | ||
| 0.20 | daq | 1.00 | 3.50 | 1.00 | ||
| Sifooyinka Farsamada | ||
| Xoogga Tijaabada | ≥410 MPa | |
| Xoogga Wax Soo Saarka | ≥200 MPa | |
| Kordhinta | ≥30% | |
| Xoogga Saamaynta | ≥100 J | |
Sifooyinka farsamoyaqaanku waa qiyaas waxayna ku kala duwanaan karaan iyadoo lagu saleynayo kulaylka, gaaska gaashaamaynta, xuduudaha alxanka iyo arrimo kale.
Gaasaska gaashaanka
TS EN ISO 14175 - TIG: I1 (Argon)
Meelaha Alxanka
TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG
| Xogta Baakaynta | |||
| Dhexroorka | Dhererka | Miisaanka | |
| 1.60 mm 2.40 mm | 1000 mm 1000 mm | 5 Kg 5 Kg | |
Mas'uuliyadda: Iyadoo dhammaan dadaallada macquulka ah la sameeyay si loo hubiyo saxnaanta macluumaadka ku jira, macluumaadkan waa la beddeli karaa iyada oo aan la ogeysiin waxaana loo tixgelin karaa oo keliya inuu ku habboon yahay hagitaan guud.