Nikkel DaawahaSilig alxankaWire Tig ahERNiCrMo-10
| Heerarka |
| TS EN ISO 18274 - Ni 6022 - NiCr21Mo13Fe4W3 |
| AWS A5.14 – ER NiCrMo-10 |
Sifooyinka iyo Codsiyada
Daawaha Nikkel-chromium-molybdenum oo loogu talagalay inuu ku biiro C22, 625, 825 ama isku-darka daawahaan.
Waxay bixisaa bir adag oo aan lahayn Nb-ka oo loogu talagalay alxanka kala duwan ee birta aan lahayn ee super austenitic iyo super duplex.
Waxay bixisaa iska caabin aad u fiican oo ka dhan ah walbahaarka iyo dildilaaca daxalka, godadka iyo daxalka daloolada.
Si ballaaran ayaa loogu isticmaalaa dahaarka iyo dahaarka birta dahaarka hoose.
Caadi ahaan waxaa loo isticmaalaa alxanka warbaahinta si xooggan u daxaleysa ee warshadaha kiimikada, duleelada u adkaysta daxalka iyo deegaannada batroolka iyo kuwa badda ee daran iwm.
Shahaadooyinka Imtixaanka waxaa laga heli karaa khadka tooska ah @wilkinsonstar247.com
Qalabka Saldhigga Caadiga ah
Daawaha 22, Daawaha 625, Daawaha 825, Daawaha 926*
* Liis tusaale ah, oo aan dhammaystirnayn
| Halabuurka Kiimikada % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | Cu% |
| ugu badan | ugu badan | 2.00 | ugu badan | ugu badan | ugu badan | ugu badan |
| 0.010 | 0.50 | 6.00 | 0.020 | 0.010 | 0.08 | 0.50 |
| Ni% | Co% | Cr% | Bisha% | V% | W% | |
| 49.00 | ugu badan | 20.00 | 12.50 | ugu badan | 2.50 | |
| daq | 2.50 | 22.50 | 14.50 | 0.30 | 3.50 | |
| Sifooyinka Farsamada | ||
| Xoogga Tijaabada | ≥690 MPa | |
| Xoogga Wax Soo Saarka | - | |
| Kordhinta | - | |
| Xoogga Saamaynta | - | |
Sifooyinka farsamoyaqaanku waa qiyaas waxayna ku kala duwanaan karaan iyadoo lagu saleynayo kulaylka, gaaska gaashaamaynta, xuduudaha alxanka iyo arrimo kale.
Gaasaska gaashaanka
TS EN ISO 14175 - TIG: I1 (Argon)
Meelaha Alxanka
TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG
| Xogta Baakaynta | |||
| Dhexroorka | Dhererka | Miisaanka | |
| 1.60 mm | |||
2.40 mm
3.20 mm1000 mm
1000 mm
1000 mm5 Kg
5 Kg
5 Kg
Mas'uuliyadda: Iyadoo dhammaan dadaallada macquulka ah la sameeyay si loo hubiyo saxnaanta macluumaadka ku jira, macluumaadkan waa la beddeli karaa iyada oo aan la ogeysiin waxaana loo tixgelin karaa oo keliya inuu ku habboon yahay hagitaan guud.