Nikkel DaawahaSilig alxankaWire Tig ahERNiCu-7
| Heerarka |
| EN ISO 18274 - Ni 4060 - NiCu30Mn3Ti |
| AWS A5.14 – ER NiCu-7 |
Sifooyinka iyo Codsiyada
Daawaha Nikkel-naxaasta ah ee loogu talagalay alxanka Monel.
Muuqasho wanaagsan oo kuul ah iyo iska caabin aad u fiican oo ku jirta xalalka milixda.
Birta alxanka waxay leedahay iska caabin aad u fiican oo ka dhan ah tiro badan oo ah warbaahinta wax burburisa.
Daawadan waxaa sidoo kale loo isticmaalaa dahaarka alxanka.
Badanaa waxaa loo isticmaalaa dhismaha badda, gaar ahaan badda, qalabka lagu beddelo kulaylka, dhuumaha, warshadaha cusbaynta, warshadaha kiimikada, kiimikada iyo injineernimada tamarta iwm.
Qalabka Saldhigga Caadiga ah
Daloolada Monel 400 iyo 404*
* Liis tusaale ah, oo aan dhammaystirnayn
| Halabuurka Kiimikada % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | |
| ugu badan | 3.00 | 0.50 | ugu badan | ugu badan | ugu badan | |
| 0.15 | 4.00 | 2.50 | 0.020 | 0.015 | 1.00 | |
| Cu% | Ni% | Co% | Ti% | Al% | Nb+Ta% | |
| 28.00 | 62.00 | ugu badan | 1.50 | ugu badan | ugu badan | |
| 32.00 | 69.00 | 1.00 | 3.00 | 1.00 | 0.50 | |
| Sifooyinka Farsamada | ||
| Xoogga Tijaabada | ≥450 MPa | |
| Xoogga Wax Soo Saarka | ≥180 MPa | |
| Kordhinta | ≥30% | |
| Xoogga Saamaynta | ≥80 J | |
Sifooyinka farsamoyaqaanku waa qiyaas waxayna ku kala duwanaan karaan iyadoo lagu saleynayo kulaylka, gaaska gaashaamaynta, xuduudaha alxanka iyo arrimo kale.
Gaasaska gaashaanka
TS EN ISO 14175 - TIG: I1 (Argon)
Meelaha Alxanka
TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG
| Xogta Baakaynta | |||
| Dhexroorka | Dhererka | Miisaanka | |
| 1.60 mm 2.40 mm 3.20 mm | 1000 mm 1000 mm 1000 mm | 5 Kg 5 Kg 5 Kg | |