Tayada wanaagsan ee la isku halleyn karo iyo sumcadda deynta oo aad u wanaagsan ayaa ah mabaadi'deenna, kuwaas oo naga caawin doona booska ugu sarreeya. Iyadoo la raacayo mabda'aaga "tayada koowaad, iibsadaha ugu sarreeya" ee Supply OEM/ODM 3 * 7mmpp/PE/PVC Balaastikada Elektrode ee Alxanka Balaastikada, Waxaan mudnaanta siineynaa tayada iyo qanacsanaanta macaamiisha, tanna waxaan raacnaa tallaabooyin adag oo xakamaynta tayada ah. Waxaan leenahay xarumo tijaabo ah oo gudaha ah halkaas oo alaabtayada lagu tijaabiyo dhinac kasta marxaladaha kala duwan ee farsamaynta. Annagoo haysanna teknoolojiyada ugu dambeeyay, waxaan macaamiisheenna u fududeyneynaa xarun wax soo saar oo gaar ah.
Tayo wanaagsan oo la isku halleyn karo iyo sumcad deymo oo aad u wanaagsan ayaa ah mabaadi'deenna, kuwaas oo naga caawin doona booska ugu sarreeya. U hoggaansanaanta mabda'aaga ah "tayada koowaad, iibsadaha ugu sarreeya" eeUlaha Alxanka Shiinaha iyo Usha PolyethyleneBadeecadaha iyo xalalku waxay leeyihiin sumcad wanaagsan oo leh qiimo tartan ah, abuur gaar ah, oo horseed u ah isbeddellada warshadaha. Shirkaddu waxay ku adkaysanaysaa mabda'a fikradda guul-guuleysiga, waxayna dhistay shabakad iib oo caalami ah iyo shabakad adeeg iib kadib.
CODSIYADA:
Alxanka birta 9% Cr-1% Mo iyo 9% Cr - 2% Mo oo loo isticmaalo korontada iyo weelka cadaadiska sare leh.
SHARAXAADA:
PA-8016-B8 waa elektarood haydarojiin hooseeya oo birta alxanka ay ka kooban tahay 9%Cr-1%Mo. Waxaa loogu talagalay birta heerkulka sare leh iyo biraha adeegyada haydarojiinta kulul, gaar ahaan warshadaha batroolka. Elektaroodku waxaa loo ansixin karaa xooggiisa sare ee la jiidi karo, adkaysigiisa wanaagsan iyo iska caabbinta kulaylka oo weyn.
OGAYSIIS KU SAABSAN ISTICMAALKA:
1. Elektroodhada ku qallaji 350-400°C ilaa hal saac ka hor isticmaalka oo elektroodhada ku kaydi 100-150°C ka dib markaad qalajiso si taxaddar leh si aad uga fogaato qoyaanka.
2. Ku dhaqan habka tallaabada dambe ama ku dhufo qaansada saxan bir ah oo yar oo loo diyaariyey ujeeddadan gaarka ah si looga hortago in godadku ay bilaabaan qaansada.
3. Qaanso-garee sida ugu macquulsan u gaabi.
4. Kuleyli 100-150°C. Heerkulka la marinayo wuu kala duwan yahay iyadoo la raacayo dhumucda saxanka iyo nooca birta la isku dhejinayo.
5. Fiiro gaar ah u yeelo inaadan dhaafin kuleylka saxda ah sababtoo ah kulaylka xad-dhaafka ah wuxuu sababaa hoos u dhaca qiimaha saameynta iyo xoogga wax-soo-saarka birta alxanka.
IV. QAYBTA KIIMIKADA CAADIGA AH EE BIRTA ALXAMDIGA (%):
| C | Si | Mn | Cr | Mo |
| 0.06 | 0.42 | 0.68 | 9.38 | 1.05 |
V. ASTAAMAHA MAKAANIKADA CAADIGA AH EE BIRTA ALXAN:
| Xoogga Tijaabada N/mm2(Ksi) | Barta Wax-soo-saarka N/mm2 (Ksi) | Kordhinta % | PWHT |
| 705 (102) | 560 (81) | 24 | 740°C x 1 saac |
VI. BOOSKA ALXANAHA: DHAMMAAN BOOSASKA
VII. CABBIRKA IYO BAAXADA HADDA LAGU TALINAYO (AC/DC+):
| Dhexroorka (mm) | 2.5 | 3.2 | 4.0 | 5.0 | |
| Dhererka (mm) | 350 | 350 | 400 | 400 | |
| Ampere | Fidsan | 55 – 85 | 90 - 130 | 130 - 180 | 180 - 240 |
| V & OH | 50 - 80 | 80 - 115 | 110 - 170 | 150 - 200 |
Tayada wanaagsan ee la isku halleyn karo iyo sumcadda deynta oo aad u wanaagsan ayaa ah mabaadi'deenna, kuwaas oo naga caawin doona booska ugu sarreeya. Iyadoo la raacayo mabda'aaga "tayada koowaad, iibsadaha ugu sarreeya" ee Supply OEM/ODM 3 * 7mmpp/PE/PVC Balaastikada Elektrode ee Alxanka Balaastikada, Waxaan mudnaanta siineynaa tayada iyo qanacsanaanta macaamiisha, tanna waxaan raacnaa tallaabooyin adag oo xakamaynta tayada ah. Waxaan leenahay xarumo tijaabo ah oo gudaha ah halkaas oo alaabtayada lagu tijaabiyo dhinac kasta marxaladaha kala duwan ee farsamaynta. Annagoo haysanna teknoolojiyada ugu dambeeyay, waxaan macaamiisheenna u fududeyneynaa xarun wax soo saar oo gaar ah.
Bixinta OEM/ODMUlaha Alxanka Shiinaha iyo Usha PolyethyleneBadeecadaha iyo xalalku waxay leeyihiin sumcad wanaagsan oo leh qiimo tartan ah, abuur gaar ah, oo horseed u ah isbeddellada warshadaha. Shirkaddu waxay ku adkaysanaysaa mabda'a fikradda guul-guuleysiga, waxayna dhistay shabakad iib oo caalami ah iyo shabakad adeeg iib kadib.