Tyue Brand Best Arc Alxanka Elektrodes AWS ENiCrFe-1 Nickel Alxanka Usha, Usha Alxanka

Sharaxaad Gaaban:

Ni307-1 (AWS ENiCrFe-1) waa elektroodh ku salaysan nikkel oo leh dahaadh yar oo soodhiyam haydarojiin ah. Isticmaal DCEP (elektroodh toos ah oo hadda ah oo togan).


Faahfaahinta Badeecada

Calaamadaha Alaabta

Elektrode-ka Alxanka Nikkel iyo Nikkel

Ni307-1                                                     

GB/T ENi6062

AWS A5.11 ENiCrFe-1

Sharaxaad: Ni307-1 waa elektroodh ku salaysan nikkel oo leh dahaadh yar oo hydrogen sodium ah. Isticmaal DCEP (elektroodh toos ah oo hadda jira oo wanaagsan). Maadaama alxanku uu ka kooban yahay Nb, birta la dhigay waxay leedahay dabacsanaan wanaagsan iyo iska caabin dildilaac.

Adeegsiga: Waxaa loo isticmaalaa alxanka birta nikkel-chromium-ka (sida UNS N06600, UNS N06601) iyo dusha sare ee birta. Waxay leedahay sifooyin alxan bir ah oo kala duwan. Waxa kale oo loo isticmaali karaa heerkul shaqeynaya oo ah 980°C, laakiin marka heerkulku ka sarreeyo 820°C, iska caabbinta oksaydhka iyo xoogga ayaa yaraan doona.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Fe

Si

Cu

Ni

Cr

Nb + Ta

S

P

Kale

≤0.08

≤3.5

≤11.0

≤0.8

≤0.5

≥62.0

13.0 ~ 17.0

0.5 ~ 4.0

≤0.015

≤0.020

≤0.50

 

Sifooyinka farsamada ee birta alxanka:

Shayga tijaabada ah

Xoogga jiidista

Mpa

Xoogga wax soo saarka

Mpa

Kordhinta

%

Dammaanad qaaday

≥550

≥360

≥27

 

 

Hadda lagu taliyay:

Dhexroorka usha

(mm)

2.5

3.2

4.0

5.0

Hadda alxanka

(A)

60 ~ 90

80 ~ 110

110 ~ 150

130 ~ 180

 

Ogeysiis:

1. Elektroodka waa in la dubo 1 saac qiyaastii 300℃ ka hor inta aan la isticmaalin alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, saliidda, biyaha, iyo wasakhda ku jirta qaybaha alxanka ka hor inta aan la alxanka. Isku day inaad isticmaasho qaanso gaaban si aad u alxanto.

 

 