Usha Alxanka Elektroodhka Birta Yar ee AWS E10015-G (J707Ni)

Sharaxaad Gaaban:

J707Ni (AWS E10015-G) waa elektarood bir ah oo leh dahaadh yar oo leh soodhiyam haydarojiin ah.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Daawaha HooseAlxanka Birta ahElektrode

J707Ni                               

GB/T E7015-G

AWS E10015-G

 

Sharaxaad: J707Ni waa elektarood bir ah oo xoog badan oo dahaar yar leh oo leh dahaar sodium oo hooseeya. Isticmaal DCEP (elektaroodka hadda tooska ah ee togan) waxaana lagu dhejin karaa dhammaan boosaska. Birta la dhigay waxay leedahay sifooyin farsamo oo wanaagsan. Marka la barbardhigo elektarood J707, astaamaha ugu muhiimsan ee J707Ni waa in adkeysiga heerkulka hooseeya iyo iska caabbinta dildilaaca si weyn loo hagaajiyay.

Codsiga: Waxaa loo isticmaalaa alxanka qaab-dhismeedka birta xoogga badan ee daawaha hooseeya ee heerarka xoogga u dhigma, sida 14MnMoVB, WEL-TEN70 iyo HW56 ee Jabbaan iyo qaab-dhismeedyada kale ee birta xoogga badan ee daawaha hooseeya.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Si

Mn

Ni

Mo

Cr

S

P

≤0.10

≤0.60

≥1.00

1.80 ~ 2.20

0.40 ~ 0.60

≤0.20

≤0.030

≤0.030

 

Sifooyinka farsamada ee birta alxanka:

 

Shayga tijaabada ah

 

Xoogga jiidista

Mpa

 

Xoogga wax soo saarka

Mpa

 

Kordhinta

%

 

Qiimaha saameynta (J)

-40℃

-50℃

 

Dammaanad qaaday

≥690

≥590

≥15

—

≥27

 

La tijaabiyay

760

630

23

140

—

 

 

Fidinta haydarojiin ee birta la dhigay: ≤4.0mL/100g (habka glycerin) 

Baarista raajada I级: Darajada I

 

Hadda lagu taliyay:

(mm)

Dhexroorka usha

2.5

3.2

4.0

5.0

(A)

Hadda alxanka

60 ~ 100

100 ~ 140

140 ~ 190

190 ~ 250

 

 

Ogeysiis:

1. Elektroodka waa in la dubo 1 saac heerkul ah 350 ~380℃ ka hor inta aan la isticmaalin alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda ku jirta qaybaha alxanka ka hor alxanka;

3. Adeegso hawlgal qaanso gaaban marka aad alxanayso. Jidka alxanka cidhiidhiga ah waa mid habboon.

 