AWS E430-16 Electrode-ka-Alxanka Birta-Aan-la'aanta ah

Sharaxaad Gaaban:

G302 (AWS E430-16) waa Cr17 ahama electrode ah oo leh daahan titanium-calcium.Waxaa loo isticmaali karaa AC iyo DC.


Faahfaahinta Alaabta

Tags Product

Alxan la'aanta BirtaElectrode

G302                                                  

GB/T E430-16

AWS E430-16 

Description: G302 waa a Cr17 ahama electrode leh daahan titanium-calcium.Waxaa loo isticmaali karaa AC iyo DC.

Codsiga: Waxaa loo isticmaalaa alxanka u adkaysta daxalka (nitric acid) iyo kulaylka u adkaysta Cr17 dhismayaasha birta aan lahayn.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.10

≤1.0

≤0.90

15.0 ~ 18.0

≤0.6

≤0.75

≤0.75

≤0.03

≤0.04

 

Qalabka makaanikada ee birta alxanka:

Shayga tijaabi

Xoog xajin

Mpa

Dheeraynta

%

La damaanad qaaday

≥450

≥20

 

Hadda lagu taliyay:

Dhexroor usheeda

(mm)

3.2

4.0

5.0

Alxanka Hadda

(A)

80 ~ 120

100 ~ 160

150 ~ 200

 

Ogaysiis:

1. electrode waa in lagu dubaa 1 saac agagaarka 150 ℃ ka hor alxanka shaqada;

2. Qaybta alxanka leh waa in lagu sii kululeeyaa 200°C ka hor alxanka.

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanaa wax soo saarka eealxanka electrodes, ulaha alxankaiyoalaabta alxankain ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.

 