AWS E6011 Ulaha alxanka

Sharaxaad Gaaban:

AWS E6011 alxanka electrode waa nooca cellulose potassium, kaas oo loo isticmaalo alxanka hoos toosan.Labadaba ee alxanka AC iyo DC.


Faahfaahinta Alaabta

Tags Product

AWS E6011alxanka electrodewaa nooca potassium cellulose, kaas oo loo isticmaalo alxanka hoos toosan.Labadaba ee alxanka AC iyo DC.Waxay qabataa tignoolajiyada shisheeye ee horumarsan waxayna leedahay sifooyin tignoolajiyadeed alxanka oo aad u wanaagsan.Dhererka ARC waa in lagu xakameeyaa si macquul ah.Ma habboona alxanka lakabyada badan iyo alxanka daboolka.

Codsiga

Ulaha alxanka AWS E6011 waxay ku habboon tahay alxanka dhismayaasha maraakiibta sida dhismayaasha iyo buundooyinka, taangiyada kaydinta, tuubooyinka iyo qalabka markabka cadaadiska.

ASTAAMAHA:

Waxtarka degdega ah ee bilawga ah

Darawalka arc sare

Slag ayaa si fudud u go'a

FAA'IIDOOYINKA QOYNEYN EE UGU WEYN:

Feedh fudud, oo ku habboon wax ka qabashada

Galid heer sare ah

Dhaqso nadiifi

Umuuqda tusbaxa siman, waxay yaraynaysaa dhabta qabow iyo goynta hoose

NOOCA hadda: Tooska ah ee Electrode Positive (DCEP) ama AC

Farsamooyinka alxanka ee lagu taliyay:

Dhererka Arc - Celceliska dhererka (1/8 "ilaa 1/4")

Flat - Ka hor marin baraf oo isticmaal dhaqdhaqaaq karbaash ah

Horizontal - Electrode xagal wax yar u jeeda saxanka sare

Kor toosan - Dharbaaxo yar ama farsamada tolitaanka

Hoosta Toosan - Isticmaal amperage sare iyo safar dheereeya, adigoo ka hor marinaya barafka

Dusha sare - Ka hor joog barafka oo isticmaal dhaqdhaqaaq karbaash ah

Halabuurka Kiimikada (%)

C Mn Si S P
<0.12 0.3-0.6 <0.2 <0.035 <0.04

Guryaha Makaanikada ee Birta La Dhigay

Shayga Tijaabada

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Qiimaha Dammaanadda

≥460

≥330

≥16

≥47

Natiijada Guud

485

380

28.5

86

Tixraaca Hadda (DC)

Dhexroorka

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40 ~ 70

50 ~ 90

90 ~ 130

130 ~ 210

170 ~ 230

Fiiro gaar ah:

1. Way fududahay in la muujiyo qoyaanka, fadlan ku hay xaalad qalalan.

2. Waxay u baahan tahay kuleyl marka xirmada jabto ama qoyaanka la nuugo, heerkulka kuleylku waa inuu u dhexeeyaa 70C ilaa 80C, wakhtiga kulaylku waa inuu ahaadaa 0.5 ilaa 1 saac.

3. Marka la isticmaalayo 5.0mm electrodes alxanka, waxa fiican in la isticmaalo cadaadis-sare, hoose- hadda, si kor loogu qaado waxqabadka alxanka.


  • Hore: