AWS E7015-G Heerkulka Hoose ee Birta Alxanka Elektrode W607 Usha Alxanka ee Haydarojiin Yar

Sharaxaad Gaaban:

W607 (AWS E7015-G) waa elektarood bir ah oo heerkul hooseeya leh oo leh dahaadh sodium ah oo hooseeya


Faahfaahinta Badeecada

Calaamadaha Alaabta

Elektrode-ka Birta Heerkulka Hoose

W607                                                     

GB/T E5015-G

AWS A5.5 E7015-G

 

Sharaxaad: W607 waa elektarood bir ah oo heerkul hoose leh oo leh dahaadh sodium oo hooseeya. Isticmaal DCEP (elektaroodka hadda tooska ah ee togan) waxaana lagu dhejin karaa dhammaan boosaska. Birta la dhigay waxay leedahay adkeysi saameyn wanaagsan oo ah -60°C.

Codsiga: Waxaa loo isticmaalaa alxanka birta heerkulka hooseeya sida 09MnD.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Sifooyinka farsamada ee birta alxanka:

Shayga tijaabada ah

Xoogga jiidista

Mpa

Xoogga wax soo saarka

Mpa

Kordhinta

%

Qiimaha saameynta (J)

-60℃

Dammaanad qaaday

≥490

≥390

≥22

≥27

 

Fidinta haydarojiin ee birta la dhigay: ≤6.0mL/100g (habka glycerin) ama ≤10mL/100g (habka mercury ama gaaska chromatography)

Baarista raajada: Darajada I

 

Hadda lagu taliyay:

(mm)

Dhexroorka usha

2.0

2.5

3.2

4.0

5.0

(A)

Hadda alxanka

40 ~ 70

60 ~ 90

100 ~ 120

140 ~ 170

170 ~ 200

 

Ogeysiis:

1. Elektroodka waa in la dubo 1 saac heerkul ah 350℃ ka hor inta aan la isticmaalin alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda ku jirta qaybaha alxanka ka hor alxanka;

3. Qaybta la alxamay waxaa lagu kululeyn karaa qiyaastii 150°C ka hor inta aan la alxamin si looga hortago dildilaaca.

 