W707Ni Heerkulka Hoose ee Birta alxanka alaab-qeybiyeyaasha alxanka

Sharaxaad Gaaban:

W707Ni waa elektrode bir heerkulka hooseeya ku jira Ni oo ku jira daahan sodium-haydaroojin hooseeya.


Faahfaahinta Alaabta

Tags Product

Birta Heerkulka HoosealxankaElectrode

W707Ni                                                     

GB/T E5515-C1

Sharaxaad: W707Ni waa kolleydh bir ah oo heerkulka hooseeya ka kooban Ni oo ku jira daahan soodhiyam hooseeya.Isticmaal DCEP (electrode toos ah oo toos ah) oo ku alxan kara dhammaan boosaska.Birta la shubay ayaa wali saameyn wanaagsan ku leh adkaanta -70°C.

Codsiga: Waxaa loo isticmaalaa alxanka birta heerkulka hooseeya sida 2.5Ni.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.60

2.00 ~ 2.75

≤0.020

≤0.025

 

Qalabka makaanikada ee birta alxanka:

Shayga tijaabi

Xoog xajin

Mpa

Xoog soo saar

Mpa

Dheeraynta

%

Qiimaha saamaynta (J)

-70 ℃

La damaanad qaaday

≥540

≥440

≥17

≥27

 

Waxyaalaha hydrogen firidhsan ee birta la shubay: ≤6.0mL/100g (hab glycerin) ama ≤10mL/100g (habka meerkuri ama gaaska chromatography)

Kormeerka raajada: Waxaan darajo

 

Hadda lagu taliyay:

(mm)

Dhexroor usheeda

2.0

2.5

3.2

4.0

5.0

(A)

Alxanka Hadda

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 Ogaysiis:

  1. Electrode waa in lagu dubaa 1 saac 350 ℃ ka hor hawlgalka alxanka;
  2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda qaybaha alxanka ka hor;
  3. Isku day inaad isticmaashid tamarta xariiqda yar markaad alxanayso, lakabyo badan iyo alxanka baasaska badan.

 