AWS E8018-C1 Heerkulka Hoose ee Birta Alxanka Elektrode W606Fe Ulaha Alxanka Haydarojiin Hoose ee ARC

Sharaxaad Gaaban:

W606Fe (AWS E8018-C1) waa elektarood bir ah oo heerkul hooseeya leh oo leh budada birta iyo dahaarka potassium-ka haydarojiin hooseeya


Faahfaahinta Badeecada

Calaamadaha Alaabta

Heerkulka HooseAlxanka Birta ahElektrode

W606Fe                                                     

GB/T E5518-C1

AWS A5.5 E8018-C1

Sharaxaad: W606Fe waa elektarood bir ah oo heerkul hooseeya leh oo leh budada birta iyo dahaarka potassium-ka haydarojiin hooseeya. Waxaa loo isticmaali karaa alxanka booska oo dhan leh AC iyo DC. Birta la dhigay waxay leedahay adkeysi saameyn wanaagsan leh -60°C. 

Codsiga: Waxaa loo isticmaalaa alxanka birta heerkulka hooseeya sida 2.5Ni.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Ni

S

P

≤0. 12

≤1.25

≤0.80

2.00 ~ 2.75

≤0.020

≤0.025

 

Sifooyinka farsamada ee birta alxanka:

Shayga tijaabada ah

Xoogga jiidista

Mpa

Xoogga wax soo saarka

Mpa

Kordhinta

%

Qiimaha saameynta (J)

-60℃

Dammaanad qaaday

≥540

≥440

≥17

≥27

 

Fidinta haydarojiin ee birta la dhigay: ≤6.0mL/100g (habka glycerin) ama ≤10mL/100g (habka mercury ama gaaska chromatography)

Baarista raajada: Darajada I

 

Hadda lagu taliyay:

(mm)

Dhexroorka usha

3.2

4.0

5.0

(A)

Hadda alxanka

90 ~ 120

140 ~ 180

180 ~ 210

 

Ogeysiis:

1. Elektroodka waa in la dubo 1 saac heerkul ah 350℃ ka hor hawlgalka alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda ku jirta qaybaha alxanka ka hor inta aan la alxanka.

 