AWS ER347 Xargaha Alxanka ee Birta Aan-Aabaha ahayn MIG iyo TIG Alxanka Ulaha Buuxinta

Sharaxaad Gaaban:

Xakamaynta alxanka birta ah waxay leedahay hufnaan sare oo alxanka, waxqabadka farsamada alxanka wanaagsan ee alxanka booska oo dhan.Waxaa si weyn loogu isticmaalaa warshadaha: dhismayaasha dhismaha, gaadiidka, injineernimada buundada, mashiinada macdanta, tareenka, dhuumaha saliidda, qalabka cadaadiska gaaska, qalabka korontada, iwm.


Faahfaahinta Alaabta

Tags Product

Kala soocida AWS:AWS 5.9

SHARAXA:

Xakamaynta alxanka birta ah waxay leedahay hufnaan sare oo alxanka, waxqabadka farsamada alxanka wanaagsan ee alxanka booska oo dhan.Waxaa si weyn loogu isticmaalaa warshadaha: qaab-dhismeedka dhismaha, gaadiidka, injineernimada buundada, mashiinada macdanta, tareenka, tuubada saliidda, qalabka cadaadiska-gaaska, qalabka korontada, iwm.

MUNAASADDA NO.& QAYBKA:

1. Adeegga OEM sahayda warshadda.

2. Model: ER308 ER308L ER308Lsi ER309 ER309L ER316 ER316L ER316Lsi iwm.

3. Cabbirka siliga MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4.TIG cabbirka siliga: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.

HORDHAC:

Waxaan bixinaa noocyo kala duwan oo ah silig alxanka birta ah, oo ay ku jiraan Mig adag silig alxanka, Tig rod silig alxanka hoostiisa-arc, oo dhan oo tayo sare leh oo lagu iibiyo adduunka oo dhan.

Marka laga reebo 308 iyo 309, waxaan sidoo kale bixinaa 304, 321, 347, 316L, 310, 2209, iyo 201. Sidoo kale tilmaamo gaar ah sida 318L, 904L, 2594, NiCrMo-3, Ni1.

Baakadaha:

Xirmooyinka siliga alxanka Mig (baakada iyo durbaanka)

Dhexroorka: 0.8 - 2.0mm

Xidhmada: 1 kg/spool, 5kg/spool, 15kg/spool, 20kg/spool, 100 kg/ durbaan, 200kg/ durbaan

Xirmooyinka siliga alxanka tig ul (tuubo caag ah)

Dhexroorka: 1.0 - 5.0mm

Xidhmada: 5 kg / baakidh

Silig alxanka arc quusay

Dhexroorka: 2.5 - 5.0mm

Xidhmada: 20kg / baakidh, 25 kg / baakidh

Baakadaha dhexdhexaadka ah iyo OEM waa la soo dhaweynayaa!

QAABYADA Kiimikada ee Silig-Alxanka Birta Aan-Aan Wanagsanayn:

Qaabka No.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

HANTIDA MASHINKA EE SIILKA ALxanka:

Qaabka No.

Xoog xamaasada Rm (Mpa)

Awood soo saarid Rel ama Rp0.2(Mpa)

Dheeraynta

(%)

Qaabka No.

Xoog xamaasada Rm (Mpa)

Awood soo saarid Rel ama Rp0.2(Mpa)

Dheeraynta

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

TIG iyo MIG ka samaysan silig alxanka birta ah

YB5092-2005

AWS

Halabuurka Kiimikada %

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1.80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Cu;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay sanadkii 2000. Waxaan ku hawlanaa wax soo saarka ee electrodes alxanka, ulo alxanka, iyo alxanka consumables in ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay sanadkii 2000. Waxaan ku hawlanaa wax soo saarka ee electrodes alxanka, ulo alxanka, iyo alxanka consumables in ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.


  • Hore:
  • Xiga: