AWS/ASME A 5.3 E 3003 Aluminium alxanka Electrodes

Sharaxaad Gaaban:

Wixii alxanka aluminium aluminium oo leh manganese iyo magnesium.Sidoo kale aad ugu fiican ku biirida darajooyinka kala duwan ee aluminium iyo codsiyada biyaha badda


Faahfaahinta Alaabta

Tags Product

Sabuur hoose oo leh afar khaanado, oo loogu talagalay caddaan oo leh fareem dahab ah oo qurxoon iyo lahjad, iyo muraayad cad oo daboolaysa dusha sare.Si qurux badan loo farsameeyay oo lagu daro meel kasta oo lagu noolaado.Ku fiican qof kasta oo la dhacsan alaabta guryaha casriga ah iyo kuwa raaxada leh.

Ururinta Gillmore Alberto waxay ku habboon tahay abuurayaasha gudaha gudaha raaxada & bandhigyada guryaha.

Iyada oo leh khadad casri ah oo nadiif ah oo qallafsan, tafaasiil daahsoon, qayb kastaa waa (marmar) shay heersare ah oo loogu talagalay gudaha gudaha, oo loo qaabeeyey iyadoo maskaxda lagu hayo waxtarka.Dhammaan alaabooyinka lacquered waxaa lagu heli karaa satin matt cad ama matt cawl, oo leh bir qurux badan oo ku dhejinaysa naxaas ama chrome madow si ay u muujiso muuqaal casri ah oo leh rafcaan caalami ah.

Mid ka mid ah sifooyinka gaarka ah ee ururintan ayaa ah muraayadda midabaysan ee isku midka ah ee dhammaan armaajooyinka Alberto ee taabashada waarta ee tayada aan la daboolin.Intaa waxaa dheer, ikhtiyaarada kaydinta deeqsinimada ah ayaa la heli karaa, maadaama cutubyadu ay yihiin modular oo lagu keenay qaybo cabbirkoodu wax ku ool ah si loo yareeyo walbahaarka ka yimaada gaadiidka iyo rakibidda.


DIN: 1732: EL Si-Al Mn

MEESHA & CODSIGA:

Wixii alxanka aluminium aluminium oo leh manganese iyo magnesium.Sidoo kale aad ugu fiican ku biirida darajooyinka kala duwan ee aluminium iyo codsiyada biyaha badda.

Aluminium arc alxanka elektrode oo leh slag is-qaadis gaar ah.Waxa kale oo jira darajooyin kale oo aluminium ah sida 12% Si, 5% Si iyo E 1100, iwm.

Is-qaadis gaar ah

Neefka saafiga ah ee nolosha shelf dheer ee dahaarka qulqulka leh ee dahaarka leh ayaa dhaafsiisan alaabada caadiga ah ee iska caabinta qoyaanka.

Waxaa lagu soo saari karaa midabyo gaar ah oo kala duwan.

Waxaa lagu heli karaa daasadaha giraanta jiida ee PURE ALUMINUM ee hermetically u xiran ama faakiyuum bacaha bireedyada ka buuxaan ee nolosha shelf dheer.

DHAMMAAN falanqeynta birta alxanka leh (Miisaanka caadiga ah%):

Midabka Flux: Midabka Caddaan ama Gaarka ah

Si Cu Fe Zn Mn Be Zr Ti Al
0.14 .07 0.23 .002 1.3 .0001 .0004 .009 Bal.

HANTIDA MACAN EE CAADIGA AH:

Birta alxanka ee aan milmin Qiimaha ugu badan ilaa

Xoogga Jilitaanka 34,000 psi (250 N/MPa)

Xoogga Wax-soosaarka 20,000 psi (150 N/MPa)

Kordhinta 10%

Alxanka Hadda & Tilmaamaha:

Hadda Lagu Taliyo: DC Reverse (+)
Dhexroorka (mm) 3/32 (2.5) 1/8 (3.25)
Amperage ugu yar 50 70
Amperage ugu badnaan 80 120

Farsamooyinka alxanka: Ku bilow adiga oo isticmaalaya qaybta sare ee kala duwanaanshaha amperage.Si degdeg ah u quudi korantada oo si degdeg ah u dhaqaaq adigoo ilaalinaya faraqa aadka ugu dhow.

Goobaha alxanka: Flat, Horizontal

Heerarka dhigaalka:

Dhexroor (mm) Dhererka (mm) Weldmetal/Electrode Electrodesper lb (kg) ee Weldmetal Wakhtiga Depositionmin/lb (kg) AmperageSettings Heerka Soo kabashada
3/32 (2.5) 14 "(350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14 "(350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14 "(350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

XADHIGIDDA ELECTRODE KU DHAQAN & CABIRKA:

Dhexroorka (mm) 3/32 (2.5) 1/8 (3.25) 5/32 (4.0)
Dhererka (mm) 14 "(350) 14 "(350) 14 "(350)
Electrodes / lb 49 33 23
Electrodes / kg 108 73 51