Sharaxaad Gaaban:

Waxaa loo habeeyay alxanka booska, labadaba toosan iyo tuubooyin go'an oo u qalma ASME 5G ama 6G boosaska alxanka (tuubbada sida caadiga ah> dhexroorka 150mm,> 15mm darbiga).
Si fudud oo dhan weldability booska


Faahfaahinta Alaabta

Tags Product

AWS Fasalka E2209T1-1/T1-4Flux Core Wire

ASTAAMAHA
Waxaa loo habeeyay alxanka booska, labadaba toosan iyo tuubooyin go'an oo u qalma ASME 5G ama 6G boosaska alxanka (tuubada sida caadiga ah> dhexroorka 150mm,> darbiga 15mm).
Si fudud oo dhan weldability booska
Ka saarida slag heer sare ah

Gaaska gaashaanka
80% Argon / 20% CO2
100% CO2

Astaamaha Muhiimka ah
• Si siman dhammaan weldability booska
• Baakad xiran oo faaruq ah
• Ka saarida slag heer sare ah
• Shahaado muujinaysa ka kooban dhigaal, nambarka ferrite, iyo guryaha saamaynta soo jiidashada leh ee la tijaabiyay @ -196°C (-320°F)

AWS Fasalka E2209T1-1/T1-4Flux Core WireHalabuurka Kiimikada

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
AWS Fasalka E2209T1-1/T1-4 Qalabka Makaanikada ee Wire Core Flux Core
Xoogga Jilicsan 120,000 psi
Xoogga Wax-soo-saarka 95,000 psi
Kordhinta (%) 26%
AWS Class E2209T1-1/T1-4 Flux Core Parameters
Dhexroorka WFS (ipm) Amperage Volts ESO (gud.) Heerka Dhigista
(lbs/saacaddii)
.045” 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanaa wax soo saarka ee electrodes alxanka,ulaha alxanka, iyo alaabta alxanka in ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.