E2553T1-1/4 AP Xarigga Birta Dareeraha ah ee aan lahayn Birta

Sharaxaad Gaaban:

Fiilada E2553T1-4 AP flux-cored waxaa loo isticmaalaa in lagu xidho dahaarka birta aan daxalka lahayn ee laba-jibbaaran oo leh qiyaastii 25% Chromium.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Fiilo E2553T1-1/4 AP ah oo leh FLUX-CORED

KALA SOOCIDA
AWS 5.22 Fasalka E2553T1-1 iyo E2553T1-4 / ASME SFA 5.22 Fasalka E2553T1-1 iyo E2553T1-4
UNS# W39533 A#8 F#6

SHARAXAAD
E2553T1-4 waa silig fiiqan oo leh fiilooyin isku xiran oo dhan oo loogu talagalay inuu ku shaqeeyo 75% Ar / 25% CO2.
Fiiladan waxaa loogu talagalay inay si fiican uga saarto slag waxayna ku shaqeysaa wareejin globular ah oo aan lahayn dildilaac.

CODSIYADA
Fiilada E2553T1-4 AP flux-cored waxaa loo isticmaalaa in lagu xidho dahaarka birta aan daxalka lahayn ee laba-jibbaaran oo leh qiyaastii 25% Chromium.
Daloolada birta aan daxalka lahayn ee laba-jibbaaran waxay isku daraan xoog badan oo tamar iyo wax-soo-saar leh iyagoo leh iska caabin wanaagsan oo ka dhan ah godadka, daxalka, iyo dildilaaca daxalka. Shuruudahan waxaa badanaa laga helaa warshadaha badda, kiimikada, iyo batroolka.
Haddii loo baahdo qalajinta ka dib alxanka, birtan alxanka waxay u baahan doontaa heerkul sare oo ka sarreeya kan ay u baahan tahay birta salka duplex.

HABKA
Kulayl hore looma hayo. Heerkulka ugu badan ee dhex-dhexaadka ah waa 300°F.
Waxaa laga yaabaa in loo baahdo in la buufiyo si loo gaaro adkaan isku mid ah oo ku saabsan alxanka badan ee gudbaya.
Kuleylka soo galaya waa inuu ku koobnaadaa 5-40 KJ/IN.

KIIMIKADA CAADIGA AH

C Cr Ni Mo Mn Si P S N Cu
0.02 25.3 9.8 3.37 0.80 0.70 0.03 0.015 0.14 1.87

GURYAHA MAKAANIKADA CAADIGA AH

Adkeysi 25 RC sida alxanka 35 RC shaqada way adkeyd
AWOODDA TOOGASHADA 110,000 PSI Ugu Yar.
TARTAN 15% Ugu yaraan.

QAYBAHA ALXANAHA

CABBIRKA Danab AMPERAGE Gaas
.045” 25-30 130-220 75% Ar / 25% CO2 ama 100% CO2

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanayn soo saarista elektroodhada alxanka,ulaha alxanka, iyo alxanka waxyaabaha la isticmaalo in ka badan 20 sano.

Waxyaabaha ugu muhiimsan ee aan ka sameyno waxaa ka mid ah elektroodhada alxanka birta aan la saarin, elektroodhada alxanka birta kaarboon, elektroodhada alxanka birta aan la jarin, elektroodhada alxanka dusha sare, elektroodhada alxanka birta aan la jarin ee nickel & cobalt, fiilooyinka alxanka birta aan la jarin ee khafiifka ah & hoose, fiilooyinka alxanka birta aan la jarin, fiilooyinka flux ee gaaska lagu gaashaamiyay, fiilooyinka alxanka aluminium, fiilooyinka alxanka arc ee hoos yimaada, fiilooyinka alxanka nickel & cobalt ee birta, fiilooyinka alxanka naxaasta ah, fiilooyinka alxanka TIG & MIG, elektroodhada tungsten, elektroodhada kaarboon ee gouging, iyo agabyada kale ee alxanka & waxyaabaha la isticmaalo.