Heerka u dhigma
GB/T 983-2012 E410NiMo-15
AWS A5.4M-2012 E410NiMo-15
Alaab u dhiganta:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM,UNS S41500
Sharaxaad
E410NiMo-15 waa elektarood bir ah oo aan la taaban karin oo leh dahaadh yar oo hydrogen ah, oo ka kooban 11.0-12.5% Cr, 4.0-5.0% Ni, iyo 0.40-0.70% Mo. Waxay ku habboon tahay alxanka qaansada birta ee la ilaaliyo (SMAW) oo leh qaanso deggan, kala firdhis yar, iyo goyn slag oo aad u fiican. Birta la dhigay waxay bixisaa xoog sare, iska caabin wanaagsan oo daxal ah, iyo iska caabin dildilaac ah. Kuleyl hore ayaa lagu talinayaa shaqooyinka qaro weyn, daaweynta kulaylka ka dib alxanka (PWHT) waa loo baahan yahay 580 ~ 620℃ (1-2 saacadood, qaboojinta hawada, AC).
Codsiga
Ku habboon alxanka ASTM CA6NM birta la shubay, 13% Cr-4%Ni birta taxanaha ah (tusaale ahaan, Cr13Ni4Mo, Cr13Ni5Mo), iyo birta aan la taaban karin ee martensitic. Codsiyada caadiga ah waxaa ka mid ah alxanka dayactirka ee orodka marawaxadaha korontada ku shaqeeya, jirka waalka, dhuumaha cadaadiska sare leh, iyo dusha sare ee qaybaha cavitation-ka xiran. Waxaa sidoo kale loo isticmaalaa dayactirka adag ee qaybaha u adkaysta xirashada sida duubabka burburinta iyo qalabka bamka.
Halabuurka Kiimikada ee Birta Alxanka (%)
| Walax | C | Mn | Si | P | S | Cr | Ni | Mo | Cu |
| Shuruudaha | ≤0.06 | ≤1.0 | ≤0.90 | ≤0.04 | ≤0.03 | 11.0-12.5 | 4.0-5.0 | 0.40-0.70 | ≤0.75 |
| Natiijada Imtixaanka | 0.029 | 0.7 | 0.32 | 0.028 | 0.01 | 12.26 | 4.50 | 0.55 | 0.01 |
Sifooyinka Farsamada ee Birta La Dhigay
| Magaca Imtixaanka | Xoogga Laabista (Mpa) | Kordhinta% | Raajo X-Ray | Tijaabada Saamaynta, (+20℃) J | Adkaanta HB | Haydarojiin Kala-baxa (ml/100g) |
| Shuruudaha | ≥760 | ≥15 | Darajada 1aad | - | - | ≤5 |
| Natiijada Imtixaanka | 845 | 19 | Darajada 1aad | 60-90 | 250-310 | ≤5 |
Halbeegyada Alxanka ee lagu taliyay
Isha Korontada: DC Reserve (DC-)
Hadda lagu taliyay
| Dhexroorka Usha (mm) | 3.2 | 4.0 | 5.0 |
| Hadda Alxanka (A) | 80-120 | 120-160 | 150-190 |
Ogeysiis:
1. Ku kari elektaroolka 300℃ saacad ka hor intaadan isticmaalin si aad uga saarto qoyaanka.
2. Nadiifi miridhku, saliidda, iyo qoyaanka dusha sare ee birta; isticmaal hawlgal qaanso gaaban oo loogu talagalay kuul cidhiidhi ah oo alxanka ah.
3. PWHT waa in la sameeyaa isla markiiba ka dib alxanka si looga fogaado xoqidda.