Alxan la'aanta Electrode AWS A5.4 E2553-16 Dheecaan Electrodes oo leh Titanium-Kalcium Coating

Sharaxaad Gaaban:

AF2553-16 (AWS E2553-16) waa natrojiin-ka kooban duplex bir aan bir lahayn oo leh daahan titanium-calcium.


Faahfaahinta Alaabta

Tags Product

Alxan la'aanta BirtaElectrode

AF2553-16

GB/T E2553-16

AWS A5.4 E2553-16

Sharaxaad: AF2553-16 waa korantada birta ah ee duplex-ka ah ee nitrogen ka kooban oo leh daahan titanium-calcium.Waxaa loo isticmaali karaa labadaba AC iyo DC oo leh hawlqabad heer sare ah.Sababtoo ah waxa ku jira molybdenum iyo nitrogen, kaarboonku aad buu u hooseeyaa, birta kaydsan waxay leedahay iska caabin dildilaac oo wanaagsan iyo iska caabin daxalka, gaar ahaan iska caabinta daxalka.

Codsiga: Waxaa loo isticmaalaa alxanka birta laba-laaban oo leh chromium oo ku saabsan 25%, sida 022Cr25Ni7Mo4N, 03Cr25Ni6Mo3Cu2N, UNS 32550 (Alloy255), iwm.

 

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Cr

Ni

Mo

Cu

N

S

P

≤0.06

0.5 ~ 1.5

≤1.0

24.0 ~ 27.0

6.5 ~ 8.5

2.9 ~ 3.9

1.5 ~ 2.5

0.10 ~ 0.25

≤0.030

≤0.040

 

Qalabka makaanikada ee birta alxanka:

Shayga tijaabi

Xoog xajin

Mpa

Dheeraynta

%

La damaanad qaaday

≥760

≥15

 

Hadda lagu taliyay:

Dhexroor usheeda

(mm)

2.5

3.2

4.0

5.0

Alxanka Hadda

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Ogaysiis:

1. Electrode waa in lagu dubaa 1 saac agagaarka 250 ℃ ka hor alxanka;

2. Isticmaal korontada DC sida ugu badan ee suurtogalka ah, iyo hadda waa inuusan noqon mid aad u weyn si looga fogaado casaanka usha alxanka;

3. Kahor alxanka, ka saar saliidda, miridhku, miisaanka, qoyaanka iyo wasakhda kale ee dusha sare ee qaybaha alxanka.

 

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanaa wax soo saarka eealxanka electrodes, ulaha alxankaiyoalaabta alxankain ka badan 20 sano.

Badeecadahayada ugu muhiimsan waxaa ka mid ah birta aan lahaynalxanka electrodes, alxanka birta kaarboon, electrodes aluminium alxanka hoose, koronto alxanka dusha sare, nickel & cobalt daawaha alxanka electrodes, steel khafiif ah & fiilooyinka alxanka hoose, fiilooyinka alxanka ahama, gaasha-gaashaammaan fiilooyinka alxanka, fiilooyinka alxanka aluminium, arc alxanka quustay. .fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.

 

 