E71T-11 Kaarboon Bir ah oo Dareera Koronto ah oo leh Elektroodhada Alxanka ee Dareera Koronto leh

Sharaxaad Gaaban:

E71T-11 waa silig is-gaashanaya oo loo isticmaalo alxanka birta kaarboon.


Faahfaahinta Badeecada

Calaamadaha Alaabta

E71T-11 A5.20, BIIR KAARBOON AHFlux CoredElektrodes-ka Alxanka Qaanso

E71T-11 waa silig is-gaashanaya oo loo isticmaalo alxanka birta kaarboon. Uma baahna gaas gaashaan ah waxaana loo isticmaali karaa hawlgallo xaddidan oo alxan badan leh.

Codsiyada Caadiga ah: alxanka dabada, wareega iyo fillet-ka ee birta 16-ga ah ilaa ½"; alxanka isku-dubaridka iyo dayactirka; qaybaha mashiinka, taangiyada, dhismaha hore loo sameeyay

Fasalka AWS: E71T-11 Shahaadada: AWS A5.20/A5.20M:2005
Daawaha: E71T-11 AWS/ASME SFA A5.20

 

Booska Alxanka:
H, F, V-up, O
Hadda:
DCEN

 

Xoogga jiidista, kpsi: 70-95
Xoogga Wax Soo Saarka, kpsi: 58 daqiiqo
Kordhinta boqolkiiba: 20 daqiiqo

Kiimikada Wire-ka Caadiga ah sida ku xusan AWS A5.9 (qiimayaasha hal-hal ah ayaa ugu badan)

C Mn Si S P Al  
0.30 1.75 0.60 0.03 0.03 1.80  
  Halbeegyada Siliga Caadiga ah
Dhexroorka Booska Geedi socodka Amps Volts Xawaaraha Quudinta Silig
in (mm)  
.030″ 0.8 Dhammaan Boosaska FCAW 25 14 55
    Dhammaan Boosaska FCAW 125 16 225
.035″ 0.9 Dhammaan Boosaska FCAW 55 17 75
    Dhammaan Boosaska FCAW 80 19 110
    Dhammaan Boosaska FCAW 120 20 160
.045″ 1.2 Dhammaan Boosaska FCAW 115 15 105
    Dhammaan Boosaska FCAW 130 16 125
    Dhammaan Boosaska FCAW 160 17 170
    Dhammaan Boosaska FCAW 200 18 195
1/6" 1.6 Dhammaan Boosaska FCAW 160 17 70
    Dhammaan Boosaska FCAW 190 18 100
    Fidsan & Jiifsan FCAW 210 19 110
    Fidsan & Jiifsan FCAW 260 20 145
0.068 1.7 Dhammaan Boosaska FCAW 145 18 50
    Dhammaan Boosaska FCAW 155 18 60
    Dhammaan Boosaska FCAW 185 18 70
    Dhammaan Boosaska FCAW 240 18 100
    Fidsan & Jiifsan FCAW 255 21 111
    Fidsan & Jiifsan FCAW 315 22 160
5/64 2.0 Dhammaan Boosaska FCAW 185 16 55
    Dhammaan Boosaska FCAW 190 18 60
    Dhammaan Boosaska FCAW 220 19 70
    Fidsan & Jiifsan FCAW 26 21 90
    Fidsan & Jiifsan FCAW 315 22 124

 

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanayn soo saarista elektroodhada alxanka,ulaha alxanka, iyo alxanka waxyaabaha la isticmaalo in ka badan 20 sano.

Waxyaabaha ugu muhiimsan ee aan ka sameyno waxaa ka mid ah elektroodhada alxanka birta aan la saarin, elektroodhada alxanka birta kaarboon, elektroodhada alxanka birta aan la jarin, elektroodhada alxanka dusha sare, elektroodhada alxanka birta aan la jarin ee nickel & cobalt, fiilooyinka alxanka birta aan la jarin ee khafiifka ah & hoose, fiilooyinka alxanka birta aan la jarin, fiilooyinka flux ee gaaska lagu gaashaamiyay, fiilooyinka alxanka aluminium, fiilooyinka alxanka arc ee hoos yimaada, fiilooyinka alxanka nickel & cobalt ee birta, fiilooyinka alxanka naxaasta ah, fiilooyinka alxanka TIG & MIG, elektroodhada tungsten, elektroodhada kaarboon ee gouging, iyo agabyada kale ee alxanka & waxyaabaha la isticmaalo.