ER70S2 waa silig MIG & TiG ah oo heer sare ah oo loogu talagalay alxamaynta dhammaan noocyada birta khafiifka ah iyo kuwa kaarboonka ah, iyadoo soo saarta alxam tayo leh oo leh dalool yar. Waa silig saddex-jibbaaran oo deoksaydhaysan (Zirconium, Titanium, iyo Aluminium) taasoo ka dhigaysa doorasho aad u fiican oo lagu alxameeyo miisaanka miridhku iyo warshadda. Looma baahna wax qulqul ah badeecadan.
CODSIYADA CAADIGA AH:
tuubooyinka iyo qalabka qodista badda, shaqada birta dhismaha
| Booska Alxanka: F, V, OH, H | Hadda: DCEP |
| Xoogga jiidista, kpsi: | 70 |
| Xoogga Wax Soo Saarka, kpsi: | 58 |
| Kordhinta 2"%: | 22 |
Heerka Caadiga ah ee Charpy V-Notch: 35 ft.-lb. Marka la gaaro -20 digrii F
Kiimikada Wire-ka Caadiga ah sida ku xusan AWS A5.18 (qiimayaasha hal-hal ah ayaa ugu badan)
| C | Mn | Si | P | S | Ni | Cr | Mo | V | Cu | Ti | Zr | Al | ||
| 0.07 | 0.90-1.40 | 0.40-0.70 | 0.025 | 0.035 | 0.15 | 0.15 | 0.15 | 0.03 | 0.50 | 0.05-0.15 | 0.02-0.12 | 0.05-0.15 | ||
| Halbeegyada Alxanka Caadiga ah | ||||||||||||||
| Dhexroorka | Geedi socodka | Volt | Amps | Gaaska Gaashaandhigga | ||||||||||
| in | (mm) | |||||||||||||
| .035 | (0.9) | GMAW | 28-32 | 165-200 | Buufinta Gudbinta 98% Argon+2% Ogsajiin ama 75% Argon+25% CO2 | |||||||||
| .045 | (1.2) | GMAW | 30-34 | 180-220 | Buufinta Gudbinta 98% Argon+2% Ogsajiin ama 75% Argon+25% CO2 | |||||||||
| 1/16 | (1.6) | GMAW | 30-34 | 230-260 | Buufinta Gudbinta 98% Argon+2% Ogsajiin ama 75% Argon+25% CO2 | |||||||||
| .035 | (0.9) | GMAW | 22-25 | 100-140 | Wareejinta Wareegga Gaaban 100% CO2 ama 75% Argon + 25% CO2 | |||||||||
| .045 | (1.14) | GMAW | 23-26 | 120-150 | Wareejinta Wareegga Gaaban 100% CO2 ama 75% Argon + 25% CO | |||||||||
| 1/16 | (1.6) | GMAW | 23-26 | 160-200 | Wareejinta Wareegga Gaaban 100% CO2 ama 75% Argon + 25% CO | |||||||||
| .035 | (0.9) | GTAW | 13-16 | 60-100 | 100% Argon | |||||||||
| .045 | (1.14) | GTAW | 13-16 | 70-120 | 100% Argon | |||||||||
| 1/16 | (1.6) | GTAW | 12-15 | 100-125 | 100% Argon | |||||||||
| 3/32 | (2.4) | GTAW | 15-20 | 125-175 | 100% Argon | |||||||||
| 1/8 | (3.2) | GTAW | 15-20 | 175-250 | 100% Argon | |||||||||