ERNiFe-CI Nickel Alloy Welding Wire Tig Filler Rod Mig iyo Tig Alxanka Ulaha

Sharaxaad Gaaban:

ERNiFe-CI waxaa loo isticmaalaa alxanka birta kabka ah.Birtan wax-buuxiyaha ah ayaa si aad ah loogu shaqeeyaa si ay u daboosho duubabka birta ah ee kabka ah.Waxa kale oo loo isticmaalaa in lagu hagaajiyo shubka.Heerkulka hore ee kulaylka iyo isdhaafsiga ugu yaraan 175ºC (350ºF) ayaa lagula talinayaa inta lagu jiro alxanka, taas oo la'aanteed alxanka iyo aagagga uu saameeyay kulaylku ay yeelan karaan dildilaacyo.


Faahfaahinta Alaabta

Tags Product

ERNiFe-CI waxaa loo isticmaalaa alxanka birta kabka ah.Birtan wax-buuxiyaha ah ayaa si aad ah loogu shaqeeyaa si ay u daboosho duubabka birta ah ee kabka ah.Waxa kale oo loo isticmaalaa in lagu hagaajiyo shubka.Heerkulka hore ee kulaylka iyo isdhaafsiga ugu yaraan 175ºC (350ºF) ayaa lagula talinayaa inta lagu jiro alxanka, taas oo la'aanteed alxanka iyo aagagga uu saameeyay kulaylku ay yeelan karaan dildilaacyo.

Ni 55 (AWS class aan la cayimin) waa magac ahaan 55% silig nikkel ah.Waxyaabaha ku jira nickelka hoose waxay ka dhigaysaa daawayntan mid ka dhaqaale badan Ni 99. Dhigashada alxanka badanaa waa mashiinka la awoodi karo, laakiin xaaladaha isku-darka sare, alxanku wuxuu noqon karaa mid adag oo adag in mishiinka.Badanaa waxaa loo isticmaalaa hagaajinta kabka oo leh qaybo culus ama dhumuc weyn.Marka la barbar dhigo Ni 99, alxanka lagu sameeyay 55 Ni ayaa ka xoog badan oo ka sii muqussan, kana dulqaad badan fosfooraska marka la shubayo.Waxa kale oo ay leedahay balaadhin hoose oo ka hooseeya Ni 99, taasoo keentay dildilaaca xadhkaha fiyuuska oo yar.

KA MID AH kiimiko:

NickelNi45.0-60.0%

IronFebalance

SiliconSimax 4.0%

ManganeseMn2.5%

CopperCu2.5%

CarbonCmax 2.0%

AluminiumAlmax 1.0%

HANTIDA makaanikada:

Xoog xamaasada Rm (MPa) Awood wax-soo-saarka Rp0.2 (MPa) Kordhinta A%
min.393-579 (57-84 psi) 296-434 (40-64 psi) 6-13

Foomamka Alaabada:

Alaabta

Dhexroor, mm

Dhererka, mm

Silig loogu talagalay alxanka MIG/GMAW

0.8, 1.0, 1.2, 1.6, 2.0, 2.4, 2.5, 3.2

-

Ulaha alxanka TIG/GTAW

2.0, 2.5, 3.2, 4.0, 5.0

915 - 1000

Silig loogu talagalay alxanka SAW

2.0, 2.4, 3.2, 4.0, 5.0

-

Siliga ubucda ee Electrode

2.0, 2.5, 3.20, 3.25, 4.0, 5.0

250, 300, 350, 400, 450, 500

CODSIGA:

Binary Nickel-Iron (Ni-Fe) iyo Ni-Fe Alloys alxanka adag ee ku salaysan Ni waxaa lagu bixiyaa usha alxanka iyo fiilooyinka dhererka caadiga ah ama dhererka ilaa codsiga macaamiisha.Xaaladaha adeegga caadiga ah, ka kooban kiimikooyinka ayaa lagu heli karaa maaddooyin kala duwan Ni oo la raacayo inta badan heerarka Ameerika iyo Yurub.