Sharaxaad Gaaban:

A302 (AWS E309-15) waa Cr23Ni13 bir ah oo aan lahayn daahan oo leh daahan sodium hydrogen hooseeyo.


Faahfaahinta Alaabta

Tags Product

Alxan la'aanta BirtaElectrode

A307                                      

GB/T E309-15

AWS A5.4 E309-15

Sharaxaad: A302 waa Cr23Ni13 bir aan lahayn oo leh daahan hydrogen sodium hooseeya.Isticmaal DCEP (electrode toos ah oo toos ah) oo ku alxan kara dhammaan boosaska.Birta la shubay waxay leedahay iska caabin dildilaac oo wanaagsan iyo iska caabin oksaydh.

Codsiga: Waxa loo isticmaalaa alxanka isla nooc ka mid ah birta aan lahayn, birta qaabaysan, birta chromium sare, birta manganese sare, iwm.

  

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Qalabka makaanikada ee birta alxanka:

Shayga tijaabi

 

Xoog xajin

Mpa

Dheeraynta

%

La damaanad qaaday

≥550

≥25

 

Hadda lagu taliyay:

Dhexroor usheeda

(mm)

2.0

2.5

3.2

4.0

5.0

Alxanka Hadda

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Ogaysiis:

Korodhka waa in lagu dubaa 1 saac ku dhawaad ​​150 ℃ ka hor alxanka.

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanaa wax soo saarka eealxanka electrodes, ulaha alxankaiyoalaabta alxankain ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.