TYUE E7018 ELECTRODE BIR AH OO KAARBO AH

Sharaxaad Gaaban:

Elektroodh bir ah oo hydrogen hooseeya oo budada potassium ah oo dahaaran.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Kala-soocidda:

AWS A5.1 E7018

ISO 2560-B-E4918A

GB/T 5117 E5018

Ulaha Alxanka AWS E7018 waa elektaroodh bir ah oo bir ah oo hydrogen bir ah oo leh budada potassium-ka oo hooseeya. Boorka birta ah ee ku jira dahaarka ayaa kordhiya heerka dhigaalka. Waxay leedahay adeegsi aad u wanaagsan oo u oggolaanaya inay yeelato qaanso deggan, xoq yar, ka saarista slag-ka way fududahay oo way ku milmaysaa dhammaan boosaska. Birta la dhigay waxay leedahay sifooyin farsamo oo wanaagsan oo bixiya adkeysi heerkul hoose oo aad u wanaagsan.

Halabuurka kiimikada (%)
Halabuurka Kiimikada

C

Mn

Si

S

P

Qiimaha Dammaanadda

≤0.12

≤1.60

≤0.75

≤0.035

≤0.040

Natiijada Guud

0.089

1.2

0.38

0.028

0.04

Sifooyinka farsamada ee biraha la shubay
Shayga Tijaabada

Rm (N/mm2)

Heer (N/mm2)

A (%)

KV2(J) -30°C

Qiimaha Dammaanadda

≥490

≥400

≥20

≥27

Natiijada Guud

515

430

32

156

Hadda tixraaca (DC)

Dhexroorka

φ2.5

φ3.2

φ4.0

φ5.0

Amperage-ka

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

Booska Alxanka:

PA, PB, PC, PD, PE, PF

Qoraalo:
1. Elektaroodhka waa in lagu kululeeyaa heerkulka 350°C muddo 1 saac ah. Usha horay u kululee mar kasta oo la isticmaalo.
2. Wasakhda sida miridhku, wasakhda saliidda iyo qoyaanka waa in laga nadiifiyaa shaqada.
3. Qaanso gaaban ayaa loo baahan yahay si loo sameeyo alxanka. Waddo cidhiidhi ah oo alxanka ah ayaa la door bidaa.

 

Feejignaan:

  1. Telektroodka waa in dib loo qalajiyaa 350℃-380℃1 saac ka hor alxanka.
  2. TNasashada, saliidda, biyaha iyo wasakhda kale ee aagga alxanka waa in laga saaraa ka hor inta aan la alxanka.