AWS A5.18 ER70S-6 Birta Kaarboonka Alxanka Siliga Biraha Buuxinta ee Gaaska Alxanka Arc, Fiilooyinka Adag

Sharaxaad Gaaban:

ER70S6 waa silig bir ah oo khafiif ah oo ka kooban heerar sare oo manganese iyo silikoon marka loo eego darajooyinka kale ee caadiga ah ee siliga MIG si loo soo saaro alxanka tayada sare leh marka loo isticmaalo birta wasakhaysan, saliidda leh, ama daxalaysan.


Faahfaahinta Alaabta

Tags Product

ER70S6 waa silig bir ah oo khafiif ah oo ka kooban heerar sare oo manganese iyo silikoon marka loo eego darajooyinka kale ee caadiga ah ee siliga MIG si loo soo saaro alxanka tayada sare leh marka loo isticmaalo birta wasakhaysan, saliidda leh, ama daxalaysan.Mawduuca silikoonku wuxuu kordhiyaa dareeraha barkada alxanka, sidaas darteed abuurista muuqaal bir ah oo jilicsan oo keenaysa shiidada alxanka kadib.Siligan waxa loo habeeyey si uu u bixiyo alxanka tayada raajada ee bilaa porosity-ka ah ee xoogga ugu sarreeya (sida alxanka) ee dhammaan fiilooyinka birta kaarboon ee bannaan.

Codsiyada caadiga ah: codsiyada dukaanka guud ee leh taam liidata ama daxalaystay, taarikada saliidda leh;birta wax lagu shubo ama samatabbixinta been abuurka ah;mashaariicda guriga;biraha xaashida;taangiyada;shaqada dhismaha

Heerka AWS: ER70S6

Shahaadada: AWS A5.18/A5.18M:2005

Alloy: ER70S6

ASME SFA A5.18

Goobta alxanka: F, V, OH, H

Hadda: DCEP

Xoogga Jilitaanka, kpsi:

70

Xoogga Wax-soo-saarka, kpsi:

58

Kordhinta 2"%:

22

Kiimikada Wire-ga caadiga ah sida ku cad AWS A5.18 (qiyamka kaliya ayaa ah ugu badnaan)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Halbeegyada alxanka ee caadiga ah

Dhexroorka

Habka

Volt

Xawaaraha safarka

Amps

Gaaska gaashaanka

in

(mm)

(ipm)

.035

(0.9)

GMAW

23-26

11-22

160-300

Gudbinta Wareejinta 98% Argon+2% Ogsajiinta

.045

(1.2)

GMAW

23-29

12-21

170-375

Gudbinta Wareejinta 98% Argon+2% Ogsajiinta

1/16

(1.6)

GMAW

25-31

9-19

275-475

Gudbinta Wareejinta 98% Argon+2% Ogsajiinta

.023

GMAW

14-19

10-15

30-85

Wareejinta gaaban ee wareega 98% Argon+2% ogsijiin

.030

(0.8)

GMAW

15-20

12-24

40-130

Wareejinta gaaban ee wareega 98% Argon+2% ogsijiin

.035

(0.9)

GMAW

16-25

11-40

60-235

Wareejinta gaaban ee wareega 98% Argon+2% ogsijiin

.045

(1.14)

GMAW

18-23

12-22

90-290

Wareejinta gaaban ee wareega 98% Argon+2% ogsijiin

.035

(0.9)

GTAW

12-15

N/A

60-100

100% Argon

.045

(1.14)

GTAW

13-16

N/A

70-120

100% Argon

1/16

(1.6)

GTAW

12

N/A

100-160

100% Argon

1/16- 3/32

(1.6)-(2.4)

GTAW

12

N/A

120-250

100% Argon

1/8

(3.2)

GTAW

12

N/A

150-300

100% Argon