AWS A5.23: ECM4 Wire-ka Submerged Arc Solid Wire waa elektaroodh silig bir ah oo isku-dhafan oo hooseeya oo loogu talagalay alxanka qaansada ee ku jira codsiyada xoogga sare leh. AWS A5.23: ECM4 wuxuu la kulmaa kiimikada AWS A5.23 M4, waxaana loogu talagalay heerarka xoogga jiidista ee ka sarreeya 110 ksi.


Faahfaahinta Badeecada

Calaamadaha Alaabta

SHARAXAAD:

Fiilooyin Arc Cored ah oo ku dhex jira Bir Daawaha Hoose leh

QAYBTA:

AWS A5.23: ECM4 Wire-ka Submerged Arc Solid Wire waa elektaroodh silig bir ah oo isku-dhafan oo hooseeya oo loogu talagalay alxanka qaansada ee ku jira codsiyada xoogga sare leh. AWS A5.23: ECM4 wuxuu la kulmaa kiimikada AWS A5.23 M4, waxaana loogu talagalay heerarka xoogga jiidista ee ka sarreeya 110 ksi.

CODSIGA UGU WEYN:

Adeegsiyada hal mar iyo kuwa badan oo leh qulqulka qulqulka biyaha hoostooda lagu taliyay, Biraha Daawaha Hoose ee Xoogga Sare leh, Biraha Bakhtiinta & Xakameysan, Qaybaha qalabka culus, qaybaha dhismaha, qolofka maraakiibta, biraha la shubay, weelasha kuleyliyaha iyo cadaadiska

Biraha HSLA iyo Q&T

Samaynta qaab-dhismeedka

Samaynta qalabka Jack-up

Qalabka culus ee qalabka

Alwaaxyada wiishka

ASTAAMAHA:

Fiilada birta ku xiran waxay bixin kartaa heerarka dhigaalka oo la hagaajiyay marka loo eego fiilooyinka adag ee amperages la mid ah

Fiilooyinka birta ku shaqeeya waxay bixiyaan astaamo gelinta ballaaran marka la barbar dhigo fiilooyinka adag ee cabbirrada alxanka ee la midka ah

Dhigaal xoog badan oo aad u sarreeya oo leh adkeysi heerkul hooseeya oo aad u fiican oo ku jira xaalad alxan ah

Shuruudaha kiimikada dhigaalka alxanka ayaa la mid ah kuwa fiilooyinka adag ee EM4.

KALA SOOCYADA AWS:

Iyada oo leh Flux Xaalad Tilmaamaha Kala-soocidda (Cutubyada Dhaqanka ee Mareykanka) Kala-soocidda (Cutubyada SI)
SWX 150 Sida loo alxamo A5. 23/A5 23M F11A10-ECM4-M4 F76A7-ECM4-M4
Iyada oo leh Flux %C % Mn %Si %P %S % Cu % Cr % Ni % Bisha %TI+V+Zr
SWX 150 0.06 1.45 0.27 0.012 0.010 0.06 0.31 2.25 0.47 0.02

QAYBTA KIIMIKADA EE SILIDHKA CAADIGA AH:

Iyada oo leh Flux Haydarojiin Kala Duwan
SWX 150 7.5 ml/100g

GURYAHA MAKAANIKADA CAADIGA AH:

Iyada oo leh Flux Xaalad Xoogga Tijaabada Xoogga Wax Soo Saarka Kordhinta % 2" (50 mm)
SWX 150 Sida loo alxamo 113 ksi (779 MPa) 106 ksi (731 MPa) 20%
PWHT* 104 ksi (717 MPa) 97 ksi (669 MPa) 8%

QIIMAYAASHA SAAMAYNTA CAADIGA AH EE CHARPY V-NOTCH:

Iyada oo leh Flux Xaalad Celcelis ahaan -60°F (-50°C) Celcelis ahaan -80°F (-60°C) Celcelis ahaan -100°F (-70°C)
SWX 150 Sida loo alxamo 55 ft-lbs (75 J) 60 f-bs (81 J) 45 f-Ibs (61 J)
PWHT* 57 f-lbs (77 J) 45 ft-lbs (61 J) —