E9015-B3 elektroodh alxan bir ah oo aan daawasho lahayn

Sharaxaad Gaaban:

Elektroodhada Biraha Iska Caabinta


Faahfaahinta Badeecada

Calaamadaha Alaabta

AWS: SFA 5.5 E9015-B3Elektroodhada Biraha Iska Caabinta

Elektroodka haydarojiin ee hooseeya oo 2.25Cr – 1Mo ah birta alxanka, waxay muujisaa xoog iyo iska caabin cajiib ah heerkulka sare ilaa 575C. Waxaa loo isticmaalaa alxanka 21/4 Cr-1 Mo birta u adkaysata creep-ka iyo Cr-Mo-V birta u adkaysata hydrogen cadaadiska iyo sidoo kale birta la shubay ee isku-dhafka la mid ah birta alxanka. Codsiyada caadiga ah waxaa ka mid ah dhismaha kuleyliyaha uumiga, alxanka tuubooyinka uumiga iyo kuwa kululeeyaha sare, warshadaha korontada, warshadda saliidda iyo warshadaha kiimikada.

QAYBTA KIIMIKADA EE DHAMMAAN BIRTA ALXAQA (%)

Walax C Mn Si P S Cr Mo
Boqolkiiba 0.05-0.12 0.5-0.9 ≤0.5 ≤0.030 0.022 2.0-2.5 0.9-1.2

ASTAAMAHA FARSAMADA EE DHAMMAAN BIRTA ALXAN

(PWHT: 690°C FOR 1 HR)

UTS YS Kordhinta
(MPa) (MPa) (L= 4d)%
≥590 550 ≥15

XOGTA HADDA IYO XIRMADA: DC (+)

Cabbirka (mm)

5×450

4×450

3.15 × 450

2.5 × 350

Kala duwanaanshaha Hadda (Amps)

200-250

150-190

100-140

70-100

Tirada (Pcs./Carton)

35

55

75

100

Taxaddar

1. Dib u qalaji elektroodhada heerkul ah 250-300 C muddo hal saac ah, sida ku cad habka caadiga ah ee aan kugula talineyno.

2. Isticmaal qaanso gaaban iyo kuul xarig leh.


  • Kii hore:
  • Xiga: