AWS E7014 Birta Kaarboon Alxanka Electrodes J501Fe Ulaha alxanka Birta khafiifka ah

Sharaxaad Gaaban:

J501Fe (AWS E7014) waa budo bir ah iyo nooca titanium oxide oo daboolan korantada.


Faahfaahinta Alaabta

Tags Product

Electrode alxanka Kaarboon

J501Fe

GB/T E5014

AWS A5.1 E7014

Sharaxaad: J501Fe waa budo bir ah iyo nooca titanium oxide oo daboolan korantada.Waxaa loo isticmaali karaa alxanka meel kasta oo leh AC iyo DC, hufnaanta dhigaalka waa qiyaastii 110%.

Codsiga: Loogu talagalay birta kaarboonka iyo qaab-dhismeedka birta alloy hooseeya, sida Q345 iyo maraakiibta kale, gawaarida iyo qaab dhismeedka alxanka.

Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

S

P

≤0.12

≤1.25

≤0.60

≤0.035

≤0.035

 

Qalabka makaanikada ee birta alxanka:

Shayga tijaabi

Xoog xajin

Mpa

Xoog soo saar

Mpa

Dheeraynta

%

Qiimaha saamaynta (J)

0℃

La damaanad qaaday

≥490

≥400

≥17

≥27

La tijaabiyay

520 ~ 580

≥410

17 ~ 26

50 ~ 100

 

Kormeerka raajo: darajada II

Hadda lagu taliyay:

Dhexroor usheeda

(mm)

2.0

2.5

3.2

4.0

5.0

5.8

Hadda alxanka

(A)

40 ~ 70

70 ~ 90

90 ~ 130

160 ~ 210

210 ~ 250

260 ~ 310

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay sanadkii 2000. Waxaan ku hawlanaa wax soo saarka ee electrodes alxanka, ulo alxanka, iyo alxanka consumables in ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.

 

 