Ulaha Alxanka Birta Kaarboonka ah ee ER70S-3, Biraha Buuxinta ee loogu talagalay Siligga Alxanka Qaanso ee Gaaska lagu ilaaliyo, Siligga Tig iyo Mig

Sharaxaad Gaaban:

ER70S3 waa silig MIG ah oo loogu talagalay isticmaalka alxanka birta kaarboonka badan.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Birta Buuxinta ER70S-3 ee Kaarboonka ah ee loogu talagalay Alxanka Qaanso ee Gaaska lagu ilaaliyo

ER70S3 waa silig MIG ah oo loogu talagalay ujeedo guud oo ku habboon codsiyada badan ee alxanka birta kaarboonka. Waa silig silikoon iyo manganese ah oo ka dhigaya mid aad u fiican sameynta guud ahaan. Badeecadani waxay u baahan tahay gaas gaashaan ah.

Codsiyada Caadiga ah: wax soo saarka guud, alaabta guriga ee birta ah, birta xaashida ah, wax soo saarka birta qurxinta, qalabka beeraha

Fasalka AWS: ER70S3 Shahaadada: AWS A5.18/A5.18M:2005
Daawaha: ER70S3 ASME SFA A5.18

 

Booska Alxanka: F, V, OH, H Hadda:
MIG-DCEP
TIG-DCEN

 

Xoogga jiidista, kpsi: 70
Xoogga Wax Soo Saarka, kpsi: 58
Kordhinta 2"%: 22

Kiimikada Wire-ka Caadiga ah sida ku xusan AWS A5.18 (qiimayaasha hal-hal ah ayaa ugu badan)

C Mn Si P S Ni Cr Mo V Cu
0.06-0.15 0.90-1.40 0.45-0.75 0.025 0.035 0.15 0.15 0.15 0.03 0.50
Halbeegyada Alxanka Caadiga ah
Dhexroorka Geedi socodka Volt Amps Gaaska Gaashaandhigga
in (mm)
.035 (0.9) GMAW 28-32 165-200 Buufinta Gudbinta 98% Argon+2% Ogsajiin ama 75% Argon+25% CO2
.045 (1.2) GMAW 30-34 180-220 Buufinta Gudbinta 98% Argon+2% Ogsajiin ama 75% Argon+25% CO2
1/16 (1.6) GMAW 30-34 230-260 Buufinta Gudbinta 98% Argon+2% Ogsajiin ama 75% Argon+25% CO2
.035 (0.9) GMAW 22-25 100-140 Wareejinta Wareegga Gaaban 100% CO2 ama 75% Argon + 25% CO2
.045 (1.2) GMAW 23-26 120-150 Wareejinta Wareegga Gaaban 100% CO2 ama 75% Argon + 25% CO
1/16 (1.6) GMAW 23-26 160-200 Wareejinta Wareegga Gaaban 100% CO2 ama 75% Argon + 25% CO
1/16 (1.6) GTAW 12-15 100-125 100% Argon