Tig and Mig Wire A5.28 ER80S-D2, Biraha buuxinta daawaha hooseeya ee alxanka gaashaadka gaaska

Sharaxaad Gaaban:

ER80S-D2 waa silig bir khafiif ah oo adag oo loo isticmaalo xaaladaha porosity waa dhibaato ama marka ay tahay inaad ka hortagto baaruud-sare ama kaarboonka ku jira birtaada salka.


Faahfaahinta Alaabta

Tags Product

A5.28 ER80S-D2, Biraha buuxinta daawaha hoose ee alxanka gaashaadka

ER80S-D2 waa silig bir khafiif ah oo adag oo loo isticmaalo xaaladaha porosity waa dhibaato ama marka ay tahay inaad ka hortagto baaruud-sare ama kaarboonka ku jira birtaada salka.Waxay ka kooban tahay heerar sare oo manganese iyo silicon si ay u bixiyaan qoynta wanaagsan iyo sidoo kale miridhku iyo dulqaadka miisaanka wanaagsan.

Codsiyada caadiga ah: Codsiyada tayada raajada, alxanka awoodda sare leh, kululeeyaha uumiga, taangiyada cadaadiska, tuubooyinka gaaska, kulaylka beddelka, warshadaha petrochemical

Heerka AWS: ER80S-D2 Shahaadada: AWS A5.28/A5.28M:2005
Alloy: ER80S-D2 AWS/ASME SFA A5.28

 

Goobta alxanka: F, V, OH, H Hadda:
GMAW-DCEP

 

Xoogga Jilitaanka, kpsi: 80 daqiiqo
Xoogga Wax-soo-saarka, kpsi: 68 daq
Kordhinta %: 17 daq

Kiimikada Wire-ga caadiga ah sida ku cad AWS A5.28 (qiyamka kaliya ayaa ah ugu badnaan)

C Mn Si P S Ni Mo Cu Mid kale
0.07-0.12 1.60-2.10 0.50-0.80 0.025 0.025 0.15 0.40-0.60 0.50 0.50
Halbeegyada alxanka ee caadiga ah
Dhexroorka Habka Volt Amps Gaaska gaashaanka
in (mm)
.035 (0.9) GMAW 28-32 165-200 Xawilaadda buufinta 98% Argon/2% Ogsajiinta
.045 (1.2) GMAW 30-34 180-220 Xawilaadda buufinta 98% Argon/2% Ogsajiinta
1/16 (1.6) GMAW 30-34 230-260 Xawilaadda buufinta 98% Argon/2% Ogsajiinta
.035 (0.9) GMAW 22-25 100-140 Wareejinta gaaban ee wareega 90% Helium/ 75% Argon / 25% CO2
.045 (1.2) GMAW 23-26 120-150 Wareejinta gaaban ee wareega 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) GMAW 23-26 160-200 Wareejinta gaaban ee wareega 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon

 