J557SLA, J557SLB Usha alxanka Haydaroojin Hoose AWS E8015-G

Sharaxaad Gaaban:

Kani waa sodium hydrogen hoose ah oo dabooshay elektrode gaar ah oo loogu talagalay birta aluminiumka ah.


Faahfaahinta Alaabta

Tags Product

Electrode alxanka Alloy Low

J557SLA, J557SLB                                        

GB/T E5515-G

AWS E8015-G

Sharaxaad: Kani waa soodhiyam haydaroojin hooseeya oo daboosha elektirode gaar ah oo loogu talagalay birta aluminiumka ah.Isticmaal DCEP (electrode toos ah oo toos ah), waxaana lagu alxan karaa dhammaan boosaska leh qalliinka fallaadha gaaban.J557SLA si toos ah ayaa loo alxan karaa iyada oo aan la saarin lakabka aluminium ee dusha jeexdin ka hor alxanka.Laakiin J557SLB waa in ay ka saartaa lakabka aluminiumka ah ee dusha sare ee jeexdin ka hor alxanka.

Codsiga: Waxaa loo isticmaalaa alxanka qaab-dhismeedka birta aluminium ee hoos yimaada dhexdhexaadinta daxalka ee hydrogen sulfide, sulfur, ammonia, ammonium bicarbonate iyo nitrogen nitrogen leh heerkulka shaqada ee ka hooseeya 540 ° C.Sida tuubooyinka kululeeyaha, qalabka sifaynta batroolka, qalabka bacriminta iyo tubooyinka uumiga, iwm.

 Halabuurka kiimikada ee birta alxanka (%):

C

Mn

Si

Cr

Mo

Al

S

P

≤0.12

0.50 ~ 0.90

≤0.50

≈0.80

≥0.20

≤0.055

≤0.035

≤0.035

 Qalabka makaanikada ee birta alxanka:

Shayga tijaabi

Xoog xajin

Mpa

Xoog soo saar

Mpa

Dheeraynta

%

Qiimaha saamaynta (J)

Heerkulka caadiga ah

La damaanad qaaday

≥540

≥440

≥17

≥49

 

Mawduuca hydrogen firidhsan ee birta kaydsan: ≤6.0mL/100g (hab glycerin)

 

Kormeerka raajada: Waxaan darajo

 

Hadda lagu taliyay:

(mm)

Dhexroor usheeda

2.5

3.2

4.0

5.0

(A)

Alxanka Hadda

50 ~ 80

80 ~ 110

130 ~ 170

160 ~ 200

 

Ogaysiis:

1. Electrode waa in lagu dubaa 1 saac agagaarka 350 ℃ ka hor alxanka;

2. Waa lagama maarmaan in la nadiifiyo miridhku, miisaanka saliidda, biyaha, iyo wasakhda qaybaha alxanka ka hor.