ERCuAl-A1 Naxaas Aluminium ahSilig alxankawaa dahaar naxaas ah oo aan bir lahayn oo laga heli karo silig la isku dhejiyay iyo ul bir ah oo 36" ah oo aan lahayn wax lagu buuxiyo si loogu isticmaalo hababka alxanka birta-qashinka iyo gaaska tungsten-qashinka siday u kala horreeyaan.
ERCuAl-A1 Naxaas Aluminium ahSilig alxankaKaydka waxaa ugu horreyn loo isticmaalaa in lagu daboolo dusha sare ee booyadaha iyo kuwa u adkaysta xirashada oo u baahan adkaanta qiyaastii 125 BHN iyo in laga hortago daxalka gaar ahaan biyaha cusbada leh, cusbada birta ah, iyo asiidhyo badan oo si caadi ah loo isticmaalo oo leh heerar iyo heerkul kala duwan. Daawadan laguma talinayo in lagu biiro maadaama dahaarku aanu lahayn u janjeera inuu kululaado.
Silig Alxanka Aluminium ee ERCuAl-A1 ee Naxaasta ah ee Aluminium-ka ah Codsiyada siligyada Alxanka Aluminium-ka ah ee Naxaasta ah waxaa ka mid ah xaashiyaha tuubada, kuraasta waalka, jillaabyada la qaboojiyo, qalabka wax lagu riixo, warshadaha kiimikada, iyo warshadaha saxarka.
Silig alxan ah oo bir ah oo laga sameeyay aluminium-A1, guryaha jirka iyo farsamada
| Adkaha-Heerkulka | 1030℃ |
| Cufnaanta | 7.7kg/dm³ |
| Kordhinta | 40-45% |
| Dareere-Heerkulka | 1040℃ |
| Xoogga Tijaabada | 380-450N/mm² |
| Adkaanshaha Brinell | 100HB |
Xirmooyinka Fiilada Alxanka ee Naxaasta ah ee ERCUAL-A1 ALUMINUM
| MIG | Dhexroorka | 0.8 – 2.0mm | Baakad | D100mm D200mm D300mm | Miisaanka | 1kg/5kg/12.5kg/13.6kg/15kg |
| 0.030″-5/64″ | 2lb/10lb/27lb/30lb/33lb | |||||
| TIG | Dhexroorka | 1.6 - 6.4mm | Dhererka | 457mm / 914mm | Baakad | 5kg/sanduuq 25kg/sanduuq 10kg/xirmo balaastig ah |
| 1/16″ – 1/4″ | 18″ / 36″ | 10lb/sanduuq 50lb/sanduuq 10kg/xirmo balaastig ah |
Fadlan ogow: Badeecadaha alwaaxa ee 500lb ah ayaa la heli karaa marka la codsado.
Fiilo alxan oo Aluminium ah oo NAXARIIS ah oo isku jira (%)
| Heerka Caadiga ah | ISO24373 | GB/T9460 | GB/T9460 | BS EN14640 | AWS A5.7 | DIN 1733 |
| Fasalka | Cu6100 | SCu6100 | SCu6100A | Cu6100 | C61000 | 2.0921 |
| Daawaha | CuAl7 | CuAl7 | CuAl8 | CuAl8 | ERCUAl-A1 | SG-CuAl8 |
| Cu | bal. | bal. | bal. | bal. | bal. | bal. |
| Al | 6.0-8.5 | 6.0-8.5 | 7.0-9.0 | 6.0-9.5 | 6.0-8.5 | 7.5-9.5 |
| Fe | - | - | ugu badnaan 0.5 | 0.5 | - | ugu badnaan 0.5 |
| Mn | 0.5 | ugu badnaan 0.5 | ugu badnaan 0.5 | 0.5 | 0.5 | ugu badnaan 1.0 |
| Ni | - | - | ugu badnaan 0.5 | 0.8 | - | ugu badnaan 0.8 |
| P | - | - | - | - | - | - |
| Pb | 0.02 | - | ugu badnaan 0.02 | 0.02 | 0.02 | ugu badnaan 0.02 |
| Si | 0.2 | ugu badnaan 0.1 | ugu badnaan 0.2 | 0.2 | 0.1 | ugu badnaan 0.2 |
| Sn | - | - | ugu badnaan 0.1 | - | - | - |
| Zn | 0.2 | ugu badnaan 0.2 | ugu badnaan 0.2 | 0.2 | 0.2 | ugu badnaan 0.2 |
| kale | 0.4 | ugu badnaan 0.5 | ugu badnaan 0.2 | 0.4 | 0.5 | ugu badnaan 0.4 |
Shirkadda Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay 2000. Waxaan ku hawlanayn soo saarista elektroodhada alxanka, ulaha alxanka, iyo waxyaabaha la isticmaalo ee alxanka in ka badan 20 sano.
Waxyaabaha ugu muhiimsan ee aan ka sameyno waxaa ka mid ah elektroodhada alxanka birta aan la saarin, elektroodhada alxanka birta kaarboon, elektroodhada alxanka birta aan la jarin, elektroodhada alxanka dusha sare, elektroodhada alxanka birta aan la jarin ee nickel & cobalt, fiilooyinka alxanka birta aan la jarin ee khafiifka ah & hoose, fiilooyinka alxanka birta aan la jarin, fiilooyinka flux ee gaaska lagu gaashaamiyay, fiilooyinka alxanka aluminium, fiilooyinka alxanka arc ee hoos yimaada, fiilooyinka alxanka nickel & cobalt ee birta, fiilooyinka alxanka naxaasta ah, fiilooyinka alxanka TIG & MIG, elektroodhada tungsten, elektroodhada kaarboon ee gouging, iyo agabyada kale ee alxanka & waxyaabaha la isticmaalo.