RBCuZn-B (Nickel Bronze) Filler Biraha Alxanka

Sharaxaad Gaaban:

RBCuZn-B Nickel Bronze (RBCuZn-B) birta buuxinta birta waxay la mid tahay bronze-ka badda laakiin waxaa ku jira manganese iyo birta kuwaas oo kordhiya adkaanta iyo xoogga kaydka alxanka.


Faahfaahinta Alaabta

Tags Product

RBCuZn-B Nickel Bronze (RBCuZn-B) birta buuxinta birta waxay la mid tahay bronze-ka badda laakiin waxaa ku jira manganese iyo birta kuwaas oo kordhiya adkaanta iyo xoogga kaydka alxanka.Waxa kale oo ku jira nikkel hubinta qaybinta isku midka ah ee birta dhigaalka ku jirta.Olol dhexdhexaad ah ama wax yar oo oksaydheynaya iyo qulqulka nooca boric/boric waa in la isticmaalaa.

Heerka AWS: RBCuZn-B Shahaadada: AWS A5.8/A5.8M:2011
Alloy: RBCuZn-B ASME SFA A5.8

 

Booska Caqliga: H, V Xaddiga Dareenka:
1620-1800⁰F

 

Xoogga Jilitaanka, kpsi: 60-78
Kordhinta %, min: 25

 

Meesha dhalaalaysa 1620⁰F Adkeynta 1590⁰F Brinell Hardness 80-110

Kiimikada Wire-ga caadiga ah sida ku cad AWS A5.8 (qiyamka kaliya ayaa ah ugu badnaan)

Cu Zn Sn Fe Mn Ni Pb Al Si Mid kale
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay sanadkii 2000. Waxaan ku hawlanaa wax soo saarka ee electrodes alxanka, ulo alxanka, iyo alxanka consumables in ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.

 

 

 

 