Sharaxaad Gaaban:

ERCuSn-A Phos Bronze A waa naxaas naxaas-zinc ah oo ka kooban ku dhawaad ​​5% tiin iyo ilaa 0.35% fosfooraska lagu daray deoxidizer ahaan loo isticmaalo alxanka naxaasta iyo naxaasta.


Faahfaahinta Alaabta

Tags Product

RBCuZn-A Naval Bronze (RBCuZn-A) waa bir buuxinta naxaasta-zinc brazing oo ka kooban xaddi yar oo daasad ah si kor loogu qaado xoogga iyo iska caabinta daxalka ee deebaajiga alxanka.Waa doorasho wanaagsan marka sifooyinka xoogga badan ee naxaasta qiiqa hooseeya aan loo baahnayn.Aashitada borax-boric ayaa guud ahaan loo baahan yahay marka alaabtan la isku xoqayo.

Heerka AWS: RBCuZn-A Shahaadada: AWS A5.8/A5.8M:2011
Alloy: RBCuZn-A ASME SFA A5.8

 

Booska Caqliga: H, V Xaddiga Dareenka:
1330-1550F

 

Xoogga Jilitaanka, kpsi: 50
Kordhinta %, min: 30

 

Meesha dhalaalaysa 1650⁰F Adkeynta 1610⁰F Brinell Hardness 70-90

Kiimikada Wire-ga caadiga ah sida ku cad AWS A5.8 (qiyamka kaliya ayaa ah ugu badnaan)

Cu Zn Sn Pb Al Mid kale
57.0-61.0 Rem 0.25-1.00 0.05 0.01 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. waxaa la aasaasay sanadkii 2000. Waxaan ku hawlanaa wax soo saarka ee electrodes alxanka, ulo alxanka, iyo alxanka consumables in ka badan 20 sano.

Alaabooyinkayaga ugu muhiimsan waxaa ka mid ah alxanka alxanka birta ah, korantada alxanka birta kaarboon, korantada alxanka hoose ee alxanka, korantada alxanka alxanka, nickel & cobalt alxanka alxanka, birta khafiifka ah & fiilooyinka alxanka hoose, fiilooyinka alxanka birta, fiilooyinka alxanka gaaska, fiilooyinka qulqulka gaaska. fiilooyinka alxanka aluminium, alxanka arc hoostiisa.fiilooyinka alxanka ee nikkel & cobalt, fiilooyinka alxanka naxaas ah, TIG & MIG fiilooyin alxanka, tungsten electrodes, kaarboon gouging electrodes, iyo qalabka kale ee alxanka & isticmaalka.

 

 

 

 