E6010 elektroodh alxanka birta kaarboon

Sharaxaad Gaaban:

E6010 waa elektroodh sodium ah oo ka samaysan rutile-cellulosic.


Faahfaahinta Badeecada

Calaamadaha Alaabta

AWS E6010 Elektrode Bir ah oo Fudud

CODSIYADA:

Waxay ku habboon tahay alxanka qaab-dhismeedka birta kaarboon yar sida dhuumaha, dhismaha maraakiibta iyo buundada iwm.

KALA-SAARIDDA:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

SIFOOYINKA:

E6010 waa elektarood sodium ah oo nooca rutile-cellulosic ah. Waxaa lagu alxan karaa booska oo dhan (gaar ahaan booska toosan-hoos) iyadoo la adeegsanayo DC+ oo keliya. Waxay leedahay waxqabad alxan oo aad u fiican sida qaanso deggan, xoq yar, ka saarista slag fudud iyo awoodda dib-u-soo-nooleynta iwm. Xakamaynta barkadda dhalaalaysa oo ka wanaagsan, xoog qaanso oo xooggan iyo gelinta qoto dheer ee booska toosan-hoos.

QAYBTA KIIMIKADA EE DHAMMAAN BIRTA ALXAQA: (QIIMAHA %)

Alaabta C Mn Si S P Ni Cr Mo V
Shuruudaha ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Natiijooyinka Caadiga ah 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

ASTAAMAHA FARSAMADA EE DHAMMAAN BIRTA ALXAN:

Alaabta Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Shuruudaha ≥430 ≥330 ≥20 ≥27
Natiijooyinka Caadiga ah 475 400 26 80

DIGNIIN:

1. Guud ahaan, uma baahnid inaad dib u qalajiso elektroodka ka hor intaadan alxamin. Marka ay qoyaan ku dhacdo, waa in dib loogu qalajiyaa 70℃-90℃ muddo 1 saac ah.

2. Waa in laga saaraa miridhku, saliidda, biyaha iyo wasakhda kale ee aagga alxanka ka hor inta aan la alxanka.

HABKA HAWLGALKA CAADIGA AH: ( DC+)

Dhexroorka (mm) 2.5 3.2 4.0 5.0
Dhererka (mm) 300 350 400 400
Hadda (A) 50-80 60-100 100-140 140-180

BAAKAD:

5kg/sanduuq, 4 sanduuq/kartoon, 20kgs/kartoon, 50 kartoon/baakad. 21MT -26MT halkii 1X20″ FCL.

 

OEM/ODM:

Waxaan taageernaa OEM/ODM waxaana sameyn karnaa baakado iyadoo loo eegayo naqshadaada, fadlan nala soo xiriir si aad faahfaahin uga hesho.

 

Astaamaha Isticmaalka:

Qaanso aad u deggan.

Ka saarid aad u fiican oo ah slag.

Gelitaanku waa mid aan qoto dheerayn.

Iska caabin wanaagsan oo kul iyo daxal leh.

Iska caabin aad u fiican oo dildilaac ah.