Elektroodh bir ah oo kaarboon haydarojiin hooseeya E6011

Sharaxaad Gaaban:

AWS E6011elektroodh alxankawaa nooca potassium cellulose, kaas oo loo isticmaalo alxanka toosan ee hoos u socda. Labada alxanka AC iyo DC.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Codsiga
Ulaha alxanka AWS E6011 waxay ku habboon tahay qaab-dhismeedka weelasha alxanka sida dhismayaasha iyo buundooyinka, haamaha kaydinta, tuubooyinka iyo qalabka weelasha cadaadiska.

AWS E6011elektroodh alxankawaa nooc ka mid ah potassium cellulose, kaas oo loo isticmaalo alxanka toosan ee hoos u socda. Labadaba alxanka AC iyo DC. Waxay qaadataa tignoolajiyada shisheeye ee horumarsan waxayna leedahay sifooyin tignoolajiyadeed oo aad u fiican alxanka. Dhererka ARC waa in lagu xakameeyaa heer macquul ah. Ma aha alxanka lakabka badan ee saxda ah iyo alxanka daboolka.

Halabuurka Kiimikada (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Sifooyinka Farsamada ee Birta La Dhigay
Shayga Tijaabada Rm (N/mm2) Heer (N/mm2) A (%) KV2(J) 0℃
Qiimaha Dammaanadda ≥420 ≥330 ≥22 ≥47
Natiijada Guud 485 380 24 86
Hadda Tixraaca (DC)
Dhexroorka φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage-ka 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

NOOCA HADDA: Koronto Toos ah oo Toos ah (DCEP) ama AC

FARSAMADA ALXAN EE LAGU TALINAYO:

Dhererka Qaansada - Dhererka celceliska (1/8" ilaa 1/4")

Fidsan - Ka hor intaadan balli gelin oo isticmaal dhaqdhaqaaq yar oo karbaash ah

Jiifsan - Elektroodh xagal ah oo si yar ugu jeeda saxanka sare

Kor u taagan - Farsamo yar oo karbaash ama tolid ah

Hoos u Dhig - Isticmaal amperage sare iyo safar degdeg ah, adigoo ka horreeya balli

Dusha sare - Ka hor intaadan balli gelin oo isticmaal dhaqdhaqaaq yar oo karbaash ah

Feejignaan:
1. Way fududahay in qoyaanka la soo bandhigo, fadlan ku hay xaalad qalalan.
2. Waxay u baahan tahay kuleylin marka baakadu jabto ama qoyaanka la nuugo, heerkulka kuleylintu waa inuu ahaadaa inta u dhaxaysa 70C ilaa 80C, wakhtiga kuleylintu waa inuu ahaadaa 0.5 ilaa 1 saac.
3. Marka la isticmaalayo elektroodhada alxanka ee 5.0mm, waxaa fiican in la isticmaalo riix sare, koronto hoose, si loo xoojiyo waxqabadka alxanka.